Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.10 - 1.26 g/cc | 0.0397 - 0.0455 lb/in³ | Average value: 1.17 g/cc Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 1.07 - 1.26 g/cc | 0.0387 - 0.0455 lb/in³ | Average value: 1.12 g/cc Grade Count:17 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Density | 1.19 - 1.26 g/cc | 0.0430 - 0.0455 lb/in³ | Average value: 1.20 g/cc Grade Count:55 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Density | 1.23 - 1.26 g/cc | 0.0444 - 0.0455 lb/in³ | 322 Hardener |
Lord Adhesives 320 / 322 Epoxy Adhesive LORD® 320/322 adhesive is a general purpose, two component epoxy adhesive system formulated for primerless adhesion to automotive sheet molded compounds (SMC). This adhesive system also provides .. |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 6802 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 7010 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 7303 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 75/O Flexible PVC, Injection Molding for Footwear Heels, opaque surface |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 89/T Flexible PVC, Injection Molding for Transparent Technical Items Technical items |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 6612 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds MGS 91/T Medical Flexible PVC, Injection Molding Connectors and special components |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 87 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 60/AS Flexible PVC, Transparent Extrusion Food belt carriers |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 74/AL Flexible PVC, Transparent Extrusion Profiles according to CEE 90/128 |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 83 Flexible PVC, Transparent Extrusion Transparent profiles and pipes |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 5526/1 Flexible PVC, Lead Free Gaskets for frames |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 7010/K Flexible PVC, Lead Free Pipes |
|||
Density | 1.24 - 1.26 g/cc | 0.0448 - 0.0455 lb/in³ | ISO 1183 |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1184 |
Fainplast Compounds KLT 002 Flexible PVC, Insulation Transparent Cables Lead Free Transparent cables (105°C) |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1184 |
Fainplast Compounds KLT 90/UV Flexible PVC, Sheathing Transparent Cables Lead Free Transparent cables anti-UV |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds MGS 86 Medical Flexible PVC, Injection Molding Connectors and special components |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 81 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 6510/K Flexible PVC, Lead Free Pipes, UL 94 Class V1 |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 6710 Flexible PVC, Lead Free Gaskets for frames |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 7005 Flexible PVC, Lead Free Pipes and profiles |
|||
Density | 1.14 - 1.26 g/cc | 0.0412 - 0.0455 lb/in³ | Average value: 1.20 g/cc Grade Count:5 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is .. |
|||
Density | 1.22 - 1.26 g/cc | 0.0441 - 0.0455 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 65/7 Flexible PVC, Lead Free Fuses |
|||
Density | 1.24 - 1.26 g/cc | 0.0448 - 0.0455 lb/in³ | ISO 1183 |
BASF Ecovio® C2203 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |