Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 670 cc/m²/day | 43.1 cc/100 in²/day | dry; ASTM D3985 |
BASF Ecovio® C2203 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |