Polymer Property : Melting Point = 311 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 148 - 155 °C
298 - 311 °F
Pau Tai Calcium stearate, Monomer Stabilizer
Non sulfide staining and non-toxic. Excellent internal lubricity and good gelation property.Applications: Hard products, non-toxic adhesive plaster and rubber mold release
Melting Point 80.0 - 155 °C
176 - 311 °F
Average value: 120 °C Grade Count:6
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Melting Point 122 - 155 °C
252 - 311 °F
0.025" extruded film,
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester
Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti..
Melting Point 130 - 155 °C
266 - 311 °F
Huntsman/TMA
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Melting Point 145 - 155 °C
293 - 311 °F
Huntsman/TMA
Huntsman IROGRAN® A 80 P 5039 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Melting Point 110 - 155 °C
230 - 311 °F
ISO 3146
Borealis Steripeel™ WD165CF PO Compound for Sterilizable Peelable Film Applications
Steripeel WD165CF is a non-formulated film resin, specially developed for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WD165CF is suitable for various peelable..
Melting Point 110 - 155 °C
230 - 311 °F
ISO 3146
Borealis Steripeel™ WD170CF PO Compound for Sterilizable Peelable Film Applications
Steripeel WD170CF is a non-formulated film resin, specially developed for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WD170CF is suitable for various peelable..
Melting Point 135 - 155 °C
275 - 311 °F
ISO 3146
Borealis Steripeel™ WE150CF PO Compound for Sterilizable Peelable Film Applications
Steripeel WE150CF is a slip and antiblock agent formulated film resin. It is suitable for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WE150CF is suitable for..
Melting Point 145 - 155 °C
293 - 311 °F
DSC
EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 145 - 155 °C
293 - 311 °F
DSC
EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Melting Point 140 - 155 °C
284 - 311 °F
DSC
BASF Ecovio® C2224 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..
Melting Point 151 - 155 °C
304 - 311 °F
Arkema Group KYNAR® LBG2 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc.
Melting Point 137 - 155 °C
279 - 311 °F
Average value: 146 °C Grade Count:11
Overview of materials for Ethyl Cellulose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ethyl Cellulose, Molded". Each property range of values reported is minimum and maximum values of approp..
Melting Point 140 - 155 °C
284 - 311 °F
DSC
BASF Ecovio® C2203 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..