Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.280 GPa | 40.6 ksi | |
LyondellBasell Lupolen® 2410 T LDPE, Injection Molding Grade Injection moldingsData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Tensile Modulus | 0.280 GPa | 40.6 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer LUBRICOMP* YL003C is a compound based on Polyester Elastomer resin containing 15% PTFE. Added features of this grade include: Clean Compound System, Wear Resistant. |
|||
Tensile Modulus | 0.280 GPa | 40.6 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP YL003C Polyester Elastomer (Asia Pacific) LUBRICOMP* YL-4030 CCS is a PTFE Lubricated Compound based on Polyester Elastomer resin which has low ionic and low outgassing performance for the Semicon and Internal Hard Disk Drive applications. |
|||
Tensile Modulus | 0.280 GPa | 40.6 ksi | Bending Modulus; ASTM D790 |
UBE UMERIT 2000F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Tensile Modulus | 0.280 GPa | 40.6 ksi | ISO 527-1/-2 |
DSM Arnitel® PB581-H Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Modulus | 0.280 - 0.840 GPa | 40.6 - 122 ksi | ISO 527 |
BASF Ecovio® C2203 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |