Polymer Property : Water Vapor Transmission = 84.0 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 84.0 g/m²/day
5.41 g/100 in²/day
ASTM F1249
BASF Ecovio® C2203 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2203 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..