Adell AH-38 Nylon 66, 40% Mineral Filled |
Nylon 66, 40% Mineral Filled |
|
Adell AI-10 Nylon 66, Impact Modified |
Nylon 66, Impact Grade |
|
Adell AD-10 Nylon 66, Ultra High Impact |
Nylon 66, Impact Grade |
|
Adell AJ-13 Nylon 66, 15% Glass Reinforced; High Impact |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell AJ-33 Nylon 66, 15% Glass Reinforced; High Impact |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell AL-18 Nylon 66, 40% Glass Reinforced; Mineral Filled |
Nylon 66, Glass/Mineral Filled |
|
Adell AL-38 Nylon 66, 40% Glass Reinforced; Mineral Filled |
Nylon 66, Glass/Mineral Filled |
|
Adell AR-13 Nylon 66, 15% Glass Reinforced |
Nylon 66, 20% Glass Fiber Filled |
|
Adell AR-18 Nylon 66, 40% Glass Reinforced |
Nylon 66, 40% Glass Fiber Filled |
|
Adell AR-33 Nylon 66, 15% Glass Reinforced |
Nylon 66, 20% Glass Fiber Filled |
|
Adell AR-34 Nylon 66, 20% Glass Reinforced |
Nylon 66, 20% Glass Fiber Filled |
|
Adell AR-37 Nylon 66, 35% Glass Reinforced |
Nylon 66, 40% Glass Fiber Filled |
|
Adell AR-38 Nylon 66, 40% Glass Reinforced |
Nylon 66, 40% Glass Fiber Filled |
|
Adell AS-10 Nylon 66, General Purpose |
Nylon 66, Unreinforced, Flame Retardant |
|
Adell AT-13 Nylon 66, 15% Glass Reinforced; Impact Modified |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell AT-14 Nylon 66, 20% Glass Reinforced; Impact Modified |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell AT-37 Nylon 66, 35% Glass Reinforced; Impact Modified |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell AW-17 Nylon 66, 35% Glass Reinforced; Superior Finish |
Nylon 66, 40% Glass Fiber Filled |
|
Adell BD-10 Nylon 6, Ultra High Impact |
Nylon 6, Impact Grade |
|
Adell BD-30 Nylon 6, Ultra High Impact |
Nylon 6, Impact Grade |
|
Adell BH-18 Nylon 6, 40% Mineral Filled |
Nylon 6, 40% Mineral Filled |
|
Adell BH-38 Nylon 6, 40% Mineral Filled |
Nylon 6, 40% Mineral Filled |
|
Adell BI-10 Nylon 6, Impact Modified |
Nylon 6, Impact Grade |
|
Adell BI-30 Nylon 6, Impact Modified |
Nylon 6, Impact Grade |
|
Adell BJ-14 Nylon 6, 20% Glass Reinforced; High Impact |
Nylon 6, Glass Filled, Impact Grade |
|
Adell BJ-33 Nylon 6, 15% Glass Reinforced; High Impact |
Nylon 6, Glass Filled, Impact Grade |
|
Adell BJ-34 Nylon 6, 20% Glass Reinforced; High Impact |
Nylon 6, Glass Filled, Impact Grade |
|
Adell BJ-37 Nylon 6, 35% Glass Reinforced; High Impact |
Nylon 6, Glass Filled, Impact Grade |
|
Adell BL-18 Nylon 6, 40% Glass Reinforced; Mineral Filled |
Nylon 6, Glass/Mineral Reinforced |
|
Adell BL-38 Nylon 6, 40% Glass Reinforced; Mineral Filled |
Nylon 6, Glass/Mineral Reinforced |
|
Adell BR-13 Nylon 6, 15% Glass Reinforced |
Nylon 6, 20% Glass Fiber Filled |
|
Adell BR-14 Nylon 6, 20% Glass Reinforced |
Nylon 6, 20% Glass Fiber Filled |
|
Adell BR-17 Nylon 6, 35% Glass Reinforced |
Nylon 6, 40% Glass Fiber Filled |
|
Adell BR-34 Nylon 6, 20% Glass Reinforced |
Nylon 6, 20% Glass Fiber Filled |
|
Adell BR-37 Nylon 6, 35% Glass Reinforced |
Nylon 6, 40% Glass Fiber Filled |
|
Adell BR-38 Nylon 6, 40% Glass Reinforced |
Nylon 6, 40% Glass Fiber Filled |
|
Adell BS-10 Nylon 6, General Purpose |
Nylon 6, Unreinforced, Flame Retardant |
|
Adell BS-30 Nylon 6, General Purpose |
Nylon 6, Unreinforced, Flame Retardant |
|
Adell BT-13 Nylon 6, 15% Glass Reinforced; Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
|
Adell BT-33 Nylon 6, 15% Glass Reinforced; Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
|
Adell BT-37 Nylon 6, 35% Glass Reinforced; Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
|
Adell BW-37 Nylon 6, 35% Glass Reinforced; Superior Finish |
Nylon 6, 40% Glass Fiber Filled |
|
Adell DR-12 10% Glass Reinforced Polycarbonate |
Polycarbonate, 10% Glass Filled |
|
Adell EA-14 Homopolymer Polypropylene, 20% Talc Filled |
Polypropylene with 20% Talc Filler |
|
Adell EL-16 Homopolymer Polypropylene, 30% Mineral Filled; Glass Reinforced |
Polypropylene, Glass/Mineral Reinforced |
|
Adell EQ-16 Homopolymer Polypropylene, 30% Mica Filled |
Polypropylene with 30% Mica Filler |
|
Adell ER-14 Homopolymer Polypropylene, 20% Glass Reinforced |
Polypropylene with 20% Glass Fiber Filler |
|
Adell ER-18 Homopolymer Polypropylene, 40% Glass Reinforced |
Polypropylene with 40% Glass Fiber Filler |
|
Adell ER-19 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness |
Polypropylene with 40% Glass Fiber Filler |
|
Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced |
Polypropylene with 20% Glass Fiber Filler |
|
Adell ER-36 Homopolymer Polypropylene, 30% Glass Reinforced |
Polypropylene with 30% Glass Fiber Filler |
|
Adell EZ-14 Homopolymer Polypropylene, 20% Calcium Carbonate Filled |
Polypropylene with 20% Calcium Carbonate (CaCO3) Filler |
|
Adell EZ-16 Homopolymer Polypropylene, 30% Calcium Carbonate Filled |
Polypropylene with 30% Calcium Carbonate (CaCO3) Filler |
|
Adell HR-36 30% Glass Reinforced Heat Stabilized PBT |
Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled |
|
Adell RQ-14 Copolymer Polypropylene, 20% Mica Reinforced |
Polypropylene with 20% Mica Filler |
|
Adell YS-10 PC Alloy |
Polycarbonate (PC) |
|
Adell AJ-14 Nylon 66, 20% Glass Reinforced; High Impact |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell AJ-17 Nylon 66, 35% Glass Reinforced; High Impact |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell AJ-34 Nylon 66, 20% Glass Reinforced; High Impact |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell AJ-37 Nylon 66, 35% Glass Reinforced; High Impact |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell AR-14 Nylon 66, 20% Glass Reinforced |
Nylon 66, 20% Glass Fiber Filled |
|
Adell AR-17 Nylon 66, 35% Glass Reinforced |
Nylon 66, 40% Glass Fiber Filled |
|
Adell AS-30 Nylon 66, General Purpose |
Nylon 66, Unreinforced, Flame Retardant |
|
Adell AT-17 Nylon 66, 35% Glass Reinforced; Impact Modified |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell AT-34 Nylon 66, 20% Glass Reinforced; Impact Modified |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell AW-37 Nylon 66, 35% Glass Reinforced; Superior Finish |
Nylon 66, 40% Glass Fiber Filled |
|
Adell BJ-13 Nylon 6, 15% Glass Reinforced; High Impact |
Nylon 6, Glass Filled, Impact Grade |
|
Adell BR-18 Nylon 6, 40% Glass Reinforced |
Nylon 6, 40% Glass Fiber Filled |
|
Adell BR-33 Nylon 6, 15% Glass Reinforced |
Nylon 6, 20% Glass Fiber Filled |
|
Adell BT-14 Nylon 6, 20% Glass Reinforced; Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
|
Adell BT-17 Nylon 6, 35% Glass Reinforced; Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
|
Adell BT-34 Nylon 6, 20% Glass Reinforced; Impact Modified |
Nylon 6, Glass Filled, Impact Grade |
|
Adell BW-17 Nylon 6, 35% Glass Reinforced; Superior Finish |
Nylon 6, 40% Glass Fiber Filled |
|
Adell DR-16 30% Glass Reinforced Polycarbonate |
Polycarbonate, 30% Glass Filled |
|
Adell DS-10 General Purpose Polycarbonate |
Polycarbonate, Molded |
|
Adell EA-16 Homopolymer Polypropylene, 30% Talc Filled |
Polypropylene with 30% Talc Filler |
|
Adell EA-18 Homopolymer Polypropylene, 40% Talc Filled |
Polypropylene with 40% Talc Filler |
|
Adell EL-18 Homopolymer Polypropylene, 40% Mineral Filled; Glass Reinforced |
Polypropylene, Glass/Mineral Reinforced |
|
Adell EQ-14 Homopolymer Polypropylene, 20% Mica Filled |
Polypropylene with 20% Mica Filler |
|
Adell EQ-18 Homopolymer Polypropylene, 40% Mica Filled |
Polypropylene with 40% Mica Filler |
|
Adell WR-37 33% Glass Reinforced PET |
Polyethylene Terephthalate (PET), 30% Glass Reinforced |
|
Adell ZR-17 33% Glass Reinforced Nylon/Olefin Alloy |
Nylon |
|
Adell ZR-37 33% Glass Reinforced Nylon/Olefin Alloy |
Nylon |
|
Adell ZS-10 Nylon/Olefin Alloy |
Nylon |
|
Adell ZS-30 Nylon/Olefin Alloy |
Nylon |
|
Adell DR-18 40% Glass Reinforced Polycarbonate |
Polycarbonate, 40% Glass Filled |
|
Adell RA-14 Copolymer Polypropylene, 20% Talc Filled |
Polypropylene with 20% Talc Filler |
|
Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced |
Polypropylene with 30% Mica Filler |
|
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced |
Polypropylene with 20% Glass Fiber Filler |
|
Adell RR-16 Copolymer Polypropylene, 30% Glass Reinforced |
Polypropylene with 30% Glass Fiber Filler |
|
Adell RZ-14 Copolymer Polypropylene, 20% Calcium Carbonate Filled |
Polypropylene with 20% Calcium Carbonate (CaCO3) Filler |
|
Adell RZ-18 Copolymer Polypropylene, 40% Calcium Carbonate Filled |
Polypropylene with 40% Calcium Carbonate (CaCO3) Filler |
|
Adell AD-30 Nylon 66, Ultra High Impact |
Nylon 66, Impact Grade |
|
Adell AH-18 Nylon 66, 40% Mineral Filled |
Nylon 66, 40% Mineral Filled |
|
Adell AI-30 Nylon 66, Impact Modified |
Nylon 66, Impact Grade |
|
Adell AT-33 Nylon 66, 15% Glass Reinforced; Impact Modified |
Nylon 66, Glass Reinforced, Impact Grade |
|
Adell BJ-17 Nylon 6, 35% Glass Reinforced; High Impact |
Nylon 6, Glass Filled, Impact Grade |
|
Adell ER-16 Homopolymer Polypropylene, 30% Glass Reinforced |
Polypropylene with 30% Glass Fiber Filler |
|
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced |
Polypropylene with 30% Glass Fiber Filler |
|
Adell ER-38 Homopolymer Polypropylene, 40% Glass Reinforced |
Polypropylene with 40% Glass Fiber Filler |
|