Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.135 g/cc
0.04100 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 68
68
ASTM D785
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 51.7 MPa
7500 psi
ASTM D790
Flexural Modulus 4.00 GPa
580 ksi
ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
Gardner Impact 0.500 J
0.369 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 182 °C
360 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 HB
HB