Adell ER-19 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell ER-19 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 100 MPa
14500 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Strength 150 MPa
21800 psi
ASTM D790
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
0.640 J/cm

@Temperature -40.0 °C
1.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched 4.50 J/cm
8.43 ft-lb/in
ASTM D256
3.70 J/cm

@Temperature -40.0 °C
6.93 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Gardner Impact 0.800 J
0.590 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
ASTM D648