Adell EL-18 Homopolymer Polypropylene, 40% Mineral Filled; Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell EL-18 Homopolymer Polypropylene, 40% Mineral Filled; Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength, Ultimate 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 5.50 GPa
798 ksi
ASTM D790
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.30 J/cm
8.06 ft-lb/in
ASTM D256
Gardner Impact 0.600 J
0.443 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 182 °C
360 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
315 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
ASTM D648
Flammability, UL94 HB
HB