Adell RQ-14 Copolymer Polypropylene, 20% Mica Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Mica Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell RQ-14 Copolymer Polypropylene, 20% Mica Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Water Absorption 0.020 %
0.020 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 60
60
ASTM D785
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Ultimate 26.2 MPa
3800 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
5.99 ft-lb/in
ASTM D256
Gardner Impact 1.70 J
1.25 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 124 °C
255 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Flammability, UL94 HB
HB