Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785
Tensile Strength, Ultimate 165 MPa
23900 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 10.0 GPa
1450 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
305 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 149 °C
300 °F
ASTM D648