Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.035 g/cc
0.03739 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 53
53
ASTM D785
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength, Ultimate 60.7 MPa
8800 psi
ASTM D638
Elongation at Break 9.5 %
9.5 %
ASTM D638
Flexural Strength 73.1 MPa
10600 psi
ASTM D790
Flexural Modulus 3.30 GPa
479 ksi
ASTM D790
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.30 J/cm
8.06 ft-lb/in
ASTM D256
Gardner Impact 0.900 J
0.664 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: