Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell EQ-18 Homopolymer Polypropylene, 40% Mica Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Mica Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell EQ-18 Homopolymer Polypropylene, 40% Mica Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.235 g/cc
0.04462 lb/in³
ASTM D792
Water Absorption 0.040 %
0.040 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 72
72
ASTM D785
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Ultimate 32.4 MPa
4700 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 53.1 MPa
7700 psi
ASTM D790
Flexural Modulus 5.20 GPa
754 ksi
ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.10 J/cm
3.93 ft-lb/in
ASTM D256
Gardner Impact 0.300 J
0.221 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 182 °C
360 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 141 °C
286 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
ASTM D648
Flammability, UL94 HB
HB