Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell AW-37 Nylon 66, 35% Glass Reinforced; Superior Finish

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Adell Plastics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell AW-37 Nylon 66, 35% Glass Reinforced; Superior Finish.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.375 g/cc
0.04968 lb/in³
ASTM D792
Water Absorption 0.80 %
0.80 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 96
96
ASTM D785
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Ultimate 186 MPa
27000 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Strength 262 MPa
38000 psi
ASTM D790
Flexural Modulus 8.80 GPa
1280 ksi
ASTM D790
Compressive Yield Strength 221 MPa
32100 psi
ASTM D695
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: