Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Mica Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.135 g/cc
0.04100 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 66
66
ASTM D785
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength, Ultimate 28.3 MPa
4100 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 46.2 MPa
6700 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Gardner Impact 1.40 J
1.03 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 133 °C
271 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
199 °F
ASTM D648
Flammability, UL94 HB
HB