Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Water Absorption 0.22 %
0.22 %
24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 76
76
ASTM D785
Tensile Strength, Ultimate 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 122 MPa
17700 psi
ASTM D790
Flexural Modulus 3.58 GPa
519 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 141 °C
285 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ASTM D648