Adell EZ-16 Homopolymer Polypropylene, 30% Calcium Carbonate Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell EZ-16 Homopolymer Polypropylene, 30% Calcium Carbonate Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.135 g/cc
0.04100 lb/in³
ASTM D792
Water Absorption 0.040 %
0.040 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 52
52
ASTM D785
Hardness, Rockwell R 81
81
ASTM D785
Tensile Strength, Ultimate 25.5 MPa
3700 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Strength 35.8 MPa
5190 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.30 J/cm
9.93 ft-lb/in
ASTM D256
Gardner Impact 2.70 J
1.99 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 182 °C
360 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
151 °F
ASTM D648
Flammability, UL94 HB
HB