Adell AD-10 Nylon 66, Ultra High Impact

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell AD-10 Nylon 66, Ultra High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0145 cm/cm
0.0145 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 64
64
ASTM D785
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength, Ultimate 52.4 MPa
7600 psi
ASTM D638
Elongation at Break 65 %
65 %
ASTM D638
Flexural Strength 72.0 MPa
10400 psi
ASTM D790
Flexural Modulus 1.80 GPa
261 ksi
ASTM D790
Compressive Yield Strength 66.0 MPa
9570 psi
ASTM D695
Izod Impact, Notched 8.50 J/cm
15.9 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D648
Flammability, UL94 HB
HB