Processing Properties Metric English Comments
Melt Temperature 204 - 227 °C
399 - 441 °F
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene..
Melt Temperature 204 - 227 °C
399 - 441 °F
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene..
Melt Temperature 204 - 227 °C
399 - 441 °F
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o..
Melt Temperature 204 - 227 °C
399 - 441 °F
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o..
Melt Temperature 193 - 227 °C
379 - 441 °F
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro..
Melt Temperature 216 - 227 °C
420 - 441 °F
ASTM D789
Niche Polymer PA6BK Nylon 6
Information provided by Niche Polymer
Melt Temperature 216 - 227 °C
420 - 441 °F
ASTM D789
Niche Polymer PA6GF13BK Nylon 6, 13% Glass Fiber Filled
Information provided by Niche Polymer
Melt Temperature 216 - 227 °C
420 - 441 °F
ASTM D789
Niche Polymer PA6GF13N Nylon 6, 13% Glass Fiber Filled
Information provided by Niche Polymer
Melt Temperature 216 - 227 °C
420 - 441 °F
ASTM D789
Niche Polymer PA6GF43BK Nylon 6, 43% Glass Fiber Filled
Information provided by Niche Polymer
Melt Temperature 216 - 227 °C
420 - 441 °F
ASTM D789
Niche Polymer PA6GF43N Nylon 6, 43% Glass Fiber Filled
Information provided by Niche Polymer
Melt Temperature 216 - 227 °C
420 - 441 °F
ASTM D789
Niche Polymer PA6GF50BK Nylon 6, 50% Glass Fiber Filled
Information provided by Niche Polymer
Melt Temperature 216 - 227 °C
420 - 441 °F
ASTM D789
Niche Polymer PA6GM40BK Nylon 6, 40% Mineral Fiber Filled
Information provided by Niche Polymer
Melt Temperature 193 - 227 °C
379 - 441 °F
PolyOne Dynalloy™ OBC8000-T40 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8000-T40 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl..
Melt Temperature 204 - 227 °C
399 - 441 °F
PolyOne Edgetek® AT-1000 Acetal (POM) Copolymer
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melt Temperature 150 - 227 °C
302 - 441 °F
Average value: 191 °C Grade Count:79
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..
Melt Temperature 193 - 227 °C
379 - 441 °F
PolyOne Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8000-T60 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl..
Melt Temperature 210 - 227 °C
410 - 441 °F
Molding
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Melt Temperature 210 - 227 °C
410 - 441 °F
Molding
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Melt Temperature 193 - 227 °C
379 - 441 °F
Total PPR Z9421 Polypropylene, Random Copolymer, Heat Sealable Film Grade
Color/Clarity/Impact. TOTAL Petrochemicals Polypropylene Z9421 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable. The very low melting..
Melt Temperature 210 - 227 °C
410 - 441 °F
Molding
Lubrizol Estane® 2103-55D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Load bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in ..
Melt Temperature 199 - 227 °C
390 - 441 °F
Bapolene® 222F Polyethylene, Film Grade
Bapolene LL222F is a general purpose LLDPE for blown film extrusion or cast film applications. This resin offers excellent tensile and toughness properties. It is available with and without slip/a..
Melt Temperature 204 - 227 °C
399 - 441 °F
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties..
Melt Temperature 204 - 227 °C
399 - 441 °F
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene  (discontinued **)
High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen..
Melt Temperature 188 - 227 °C
370 - 441 °F
Stock
PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber  (discontinued **)
Data provided by PolyOne.
Melt Temperature 210 - 227 °C
410 - 441 °F
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer  (discontinued **)
Description: PELLETHANE® 2103-75D UV stabilized, polyether based thermoplastic polyurethane elastomer has excellent hydrolytic stability and excellent resistance to micro-organisms. Applications in..
Melt Temperature 210 - 227 °C
410 - 441 °F
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)  (discontinued **)
Description: PELLETHANE® 2104-65D Polyester based. Excellent oil and chemical resistance. Applications include: Caster wheels, Seals, Gaskets, Animal tags, Hose jacketing, Ski boots, AutomotiveDat..
Melt Temperature 210 - 227 °C
410 - 441 °F
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)  (discontinued **)
Description: PELLETHANE® 2104-45D ether-ether hybrid polyurethane elastomer has excellent low temperature properties, fast cycle time, and good resistance to fuel and oils. Applications include: C..