Borealis Borcoat™ MA115E Syntactic Polypropylene for Steel Pipe Coating

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Borealis
Trade Name Borcoat™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borcoat™ MA115E Syntactic Polypropylene for Steel Pipe Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borcoat™ MA115E is a highly filled polypropylene compound and is self colored. Applications: Borcoat™ MA115E is recommended as heavy weight coating for special applications used in steel pipe coating.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ISO 1183
Filler Content 70 %
70 %
Melt Flow 2.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
50mm/min; ISO 527-2
Elongation at Break 50 %
50 %
50mm/min; ISO 527-2
Elongation at Yield 1.8 %
1.8 %
ISO 527-2
Tensile Modulus 3.50 GPa
508 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.190 J/cm²

@Temperature 23.0 °C
0.904 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ISO 75-2
Vicat Softening Point 105 °C
221 °F
B50; ISO 306
Processing Properties Metric English Comments
Middle Barrel Temperature 200 - 220 °C
392 - 428 °F
cylinder
Die Temperature 210 - 220 °C
410 - 428 °F
Melt Temperature 210 - 230 °C
410 - 446 °F