DuPont™ Elvaloy® AC 12024S Ethylene Methyl Acrylate

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Extrusion Grade
Manufacturer DuPont
Trade Name Elvaloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Elvaloy® AC 12024S Ethylene Methyl Acrylate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvaloy® AC 12024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® AC 12024S resin complies with the U. S. Food and Drug Administration regulation 21 CFR 177.1340, Ethylene-methyl acrylate copolymer resins, for use in contact with all types of food, subject to meeting the migration limits specified in paragraph (b).
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ASTM D792, ISO 1183
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
Thermal Properties Metric English Comments
Melting Point 88.0 °C
190 °F
ASTM D3418, ISO 3146
Processing Properties Metric English Comments
Processing Temperature <= 310 °C
<= 590 °F
Feed Temperature 160 °C
320 °F
Extrusion Coating
Zone 2 210 °C
410 °F
Extrusion Coating
Zone 3 235 °C
455 °F
Extrusion Coating
Zone 4 235 °C
455 °F
Extrusion Coating
Zone 5 235 °C
455 °F
Extrusion Coating
Adapter Temperature 235 °C
455 °F
Extrusion Coating
Die Temperature 235 °C
455 °F
Extrusion Coating
Melt Temperature 210 - 260 °C
410 - 500 °F
Extrusion Coating
Users viewing this material also viewed the following: