Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PP CCP20020 UV Polypropylene, Mineral Reinforced, UV stabilized Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PP CIQ15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PP HGX500707 Polypropylene, Multifiller Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPC GF5030 PD2 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPC T16020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPC TS8030 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH GF12030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH GF3050 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH GF5020 PD1 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH GF5030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH T8038 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH TS2020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 °C | 401 °F | |
NOVA Chemicals Sclair® 31E LLDPE Extrusion Resin Features: Excellent tensile properties, excellent impact toughness, outstanding gloss and clarity, excellent processability.Applications: Coating and sheathing.Data provided by the manufacturer. |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PP TOUCH 25325 Polypropylene, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPC B10075 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH BF4075 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH BK901213 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH GF4030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH MGF5040 Polypropylene Homopolymer, Multifiller Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 245 °C | 401 - 473 °F | |
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Melt Temperature | 205 °C | 401 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 327UVE RD402 Acetal Homopolymer
(Unverified Data**) Delrin® 327UVE RD402 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Informat.. |
|||
Melt Temperature | 205 - 235 °C | 401 - 455 °F | Injection Molding |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 205 - 235 °C | 401 - 455 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 205 °C | 401 °F | Injection Molding |
Covestro Texin® 245 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Melt Temperature | 205 °C | 401 °F | |
NOVA Chemicals Sclair® 94D1 HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, high stretchability, excellent strength.Applications: Package nettings for produce, Christmas tree wrap and turkey overwrap.Data provided by the manufacturer. |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPC GF5020 Polypropylene Copolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH T5060 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH TS8038 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPHC K8040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 °C | 401 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information p.. |