Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TP-G20 Polybutylene Terephthalate, 20% Glass Reinforced Polybutylene Terephthalate, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TP-IM-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 30% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Melt Temperature | 232 - 271 °C | 450 - 520 °F | |
PTS Trimid® N6-G30L 30% GFR Lubricated Nylon 6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | Molding |
PolyOne Edgetek® PS-40GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
RTP Company RTP 4700 Polytrimethylene Terephthalate (PTT), Base Resin |
|||
Melt Temperature | 232 - 271 °C | 450 - 520 °F | |
PTS Trimid® N6-M200HL Impact Modified Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 232 - 271 °C | 450 - 520 °F | Molding |
PolyOne Edgetek® BB-20GF/000 PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | Molding |
PolyOne Edgetek® CY-10GF/000 UV FR V0 NATURAL PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedNon-HalogenatedFlame RetardantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 232 - 271 °C | 450 - 520 °F | Air purge at equilibrium conditions |
NOVA Chemicals Dylark® 520XT Glass Reinforced Engineering Resin Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
PolyOne Edgetek® NL-30GF/000 FR Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 232 - 243 °C | 450 - 469 °F | Injection Molding |
Ineos ABS Lustran® ABS 241 ABS, Blending Grade Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Melt Temperature | 232 °C | 450 °F | |
Multibase Multi-Flex® D 5308 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Melt Temperature | 232 °C | 450 °F | |
Multibase Multi-Flex® D 3104 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI.. |
|||
Melt Temperature | 232 - 274 °C | 450 - 525 °F | Oriented Film Extrusion |
Total PPH 3270 Polypropylene Homopolymer, High Crystallinity, Low Melt Flow Film Grade Low Residuals TOTAL Polypropylene 3270 utilizes the TOTAL Polypropylene proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock. 3.. |
|||
Melt Temperature | 232 - 274 °C | 450 - 525 °F | Cast Film Extrusion |
Total PPH 3576XHD Polypropylene Homopolymer, Film Grade Low Residuals TOTAL Polypropylene 3576XHD utilizes the new ATOFINA proprietary process technology to provide extremely low residuals for improved color stability and clarity.Antiblock. 3576XHD is .. |
|||
Melt Temperature | 232 - 288 °C | 450 - 550 °F | Extrusion |
Total PPH 3860X Polypropylene, Extrusion Grade High flow reactor grade homopolymer for nonwoven fibersHigh Purity - FINA 3860X features extremely high purity for processing in micro denier fibers.FDA - FINA 3860X complies with all applicable FDA.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyether Block Amide (PEBA), Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiatio.. |
|||
Melt Temperature | 232 - 249 °C | 450 - 480 °F | Nozzle temp not greater than stock |
Chi Mei Polylac® PA-765 ABS - Flame Retardant F.R. High Flow |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
RTP Company RTP 4705 UV Polytrimethylene Terephthalate (PTT), Glass Fiber - UV Stabilized |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
RTP Company RTP 4781 Polytrimethylene Terephthalate (PTT), Carbon Fiber |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
RTP Company RTP 4799 X 117571 F Polytrimethylene Terephthalate (PTT) Glass Fiber - Flame Retardant - Halogen Free |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
RTP Company RTP 4703 Polytrimethylene Terephthalate (PTT), Glass Fiber |