Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
Plastcom SLOVALEN PH 49 GF 40 PP, 40% glass fibre PP homopolymer for injection moulding, chemically strengthened with 40% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Melt Temperature | 230 - 240 °C | 446 - 464 °F | |
Polyplastic Armlen® PP MF 40-3M Polypropylene Copolymer, 40% Calcium Carbonate Injection moldingInformation provided by PolyPlastic Group. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Eastman Tenite 180A-28(HT) Cellulose Acetate
(discontinued **) 28% Plasticized.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | DAM |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | Average value: 257 °C Grade Count:19 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 230°C |
Kingfa JH960 6300 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platin.. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | ISO 294 |
Gromax BTE25-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | ISO 294 |
Gromax BTE30-FN00N1 Nylon 6 (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melt Temperature | 230 - 280 °C | 446 - 536 °F | |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
LATI Later 4 G/30-V0HF1 PBT, 30% Glass Fiber Reinforced, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe.. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
Solvay Technyl® C216V30 30% Glass Filled Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Melt Temperature | 230 °C | 446 °F | Injection molding |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Melt Temperature | 230 - 270 °C | 446 - 518 °F | Injection Molding |
Styrolution Terluran® HH-106 Q109 Colored ABS Description: Injection-molding grade with high resistance to heat deformation and impact, with improved surface quality suitable for automotive applications.Information provided by STYROLUTION, whic.. |
|||
Melt Temperature | 230 - 270 °C | 446 - 518 °F | Injection Molding |
Styrolution Terluran® HH-112 Q109 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Melt Temperature | 230 - 280 °C | 446 - 536 °F | |
Suzhou Hipro Polymers Hiprolon® 400 MC HLS G30 Nylon, 30% glass fiber filled Hiprolon® 400 MC HLS G30 is a specialty long chain polyamide compound reinforced with 30% chopped glass fiber for injection molding. It contains some bio-renewable resources Features: high dime.. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
Borealis HD120MO Polypropylene HD120MO is a polypropylene homopolymer with a good combination of mechanical properties intended for injection molding. Applications: sanitary equipment, caps and closures, and general packagingInf.. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Ecomass® 1080ZC86 Stainless Steel Powder Filled Polyamide Alloy, Injection Molding Stainless Steel Powder Filled Polyamide Alloy, Very Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shield.. |
|||
Melt Temperature | 230 °C | 446 °F | |
Eurostar Starglas FF004 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
E-Polymers TEKASTER® F101F Fast cycle time PBT Injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical performance. Specially G/F reinforced PET has excellent heat resistance, a good.. |
|||
Melt Temperature | 230 °C | 446 °F | Optimum; Extrusion |
DuPont Performance Polymers Hytrel® G5564 TPC-ET
(Unverified Data**) Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon .. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-29 MS Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.For .. |
|||
Melt Temperature | 230 - 240 °C | 446 - 464 °F | |
Celanese Celstran® PP-GF30-02 AD 3002 PP, 30% Glass Reinforced 30% long strand glass fiber reinforced polypropyleneInformation provided by Celanese |
|||
Melt Temperature | 230 - 275 °C | 446 - 527 °F | Injection molding/Extrusion |
BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF30 Polyamide 6 - Glass Fiber Reinforced 30% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF40 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 40% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 M Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 MHLS Polyamide 6 - Colored Heat and UV light stabilized grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main proper.. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | Pipe extrusion |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Celanese Celstran® PP-GF50-BV337 PP, 50% Glass Reinforced 50% long fiber glass reinforced, lubricated, heat & UV stabilized, PolypropyleneIt is normally not necessary to dry CELSTRAN PP. However, should there be surface moisture (condensate) on the molding.. |
|||
Melt Temperature | 230 - 270 °C | 446 - 518 °F | |
Plastcom SLOVASTER® B GB 40 PBT reinforced with glass beads PBT for injection molding, reinforced with 40% glass beads. Characterized by very good properties also at low temperature. Melt is characterized by very good rheology, which enables manufacturing of.. |