Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 232 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 232 - 288 °C
450 - 550 °F
Polymer Resources NY6/12-GP1 General Purpose Nylon 612
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Melt Temperature 232 - 260 °C
450 - 500 °F
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
Melt Temperature 232 - 260 °C
450 - 500 °F
Nozzle temp not greater than stock
PTS Trilac® ABS-HS4000 General Purpose ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Temperature 232 - 271 °C
450 - 520 °F
PTS Trimid® N6-200N Nylon 6 with Nucleating Agent
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Temperature 232 - 271 °C
450 - 520 °F
PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Temperature 232 - 271 °C
450 - 520 °F
PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Temperature 232 - 271 °C
450 - 520 °F
PTS Trimid® N6-G30L 30% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Temperature 232 - 271 °C
450 - 520 °F
Molding
PolyOne Lubri-Tech™ PS-30CF/10T 2S Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced, PTFE/Silicone Lubricated
Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 232 - 260 °C
450 - 500 °F
RTP Company RTP 4785 Polytrimethylene Terephthalate (PTT), Carbon Fiber
Melt Temperature 232 - 274 °C
450 - 525 °F
Average value: 257 °C Grade Count:6
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Melt Temperature 232 - 277 °C
450 - 530 °F
Molding
PolyOne Lubri-Tech™ BB-10GF/5T PC/ABS Blend, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 232 - 288 °C
450 - 550 °F
Average value: 262 °C Grade Count:8
Overview of materials for Glass Reinforced, Modified SMA
This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of..
Melt Temperature 232 - 243 °C
450 - 469 °F
Injection Molding
Ineos ABS Lustran® 750 ABS, Molding Grade
Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 bl..
Melt Temperature 232 - 243 °C
450 - 469 °F
Injection Molding
Ineos ABS Lustran® ABS 241 ABS, Blending Grade
Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v..
Melt Temperature 232 - 243 °C
450 - 469 °F
Extrusion
Ineos ABS Lustran® ABS 241 ABS, Blending Grade
Lustran® ABS 241 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v..
Melt Temperature 232 °C
450 °F
Multibase Multi-Flex® D 6606 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, GoodStiffness, Good Forms:PelletsUses: Automotive ApplicationsInformation provided by Mul..
Melt Temperature 232 °C
450 °F
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane
Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro..
Melt Temperature 232 - 277 °C
450 - 531 °F
Eastman DuraStar MN611 Polymer, Natural
Durastar Polymer MN611 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char..
Melt Temperature 232 - 260 °C
450 - 500 °F
Ecomass® 1003TU96 Tungsten Filled COPA
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by..
Melt Temperature 232 - 254 °C
450 - 490 °F
Clariant Renol PBT1100TF10 Polybutylene Terephthalate, PTFE Lubricated
Data provided by Clariant Masterbatches
Melt Temperature 232 - 249 °C
450 - 480 °F
Nozzle temp not greater than stock
Chi Mei Polylac® PA-765 ABS - Flame Retardant
F.R. High Flow
Melt Temperature 232 - 260 °C
450 - 500 °F
RTP Company RTP 4705 UV Polytrimethylene Terephthalate (PTT), Glass Fiber - UV Stabilized
Melt Temperature 232 - 260 °C
450 - 500 °F
RTP Company RTP 4709 Polytrimethylene Terephthalate (PTT), Glass Fiber
Melt Temperature 232 - 260 °C
450 - 500 °F
RTP Company RTP 4781 Polytrimethylene Terephthalate (PTT), Carbon Fiber
Melt Temperature 232 °C
450 °F
Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca..
Melt Temperature 232 - 260 °C
450 - 500 °F
RTP Company RTP 4703 Polytrimethylene Terephthalate (PTT), Glass Fiber
Copyright © lookpolymers.com All Rights Reserved