Thermal Properties Metric English Comments
CTE, linear 9.00 - 140 µm/m-°C

@Temperature >=143 °C
5.00 - 77.8 µin/in-°F

@Temperature >=289 °F
Average value: 94.8 µm/m-°C Grade Count:2
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
CTE, linear 120 - 140 µm/m-°C

@Temperature 20.0 °C
66.7 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Polimersan Plastics POLITEF® (PTFE)
POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of ..
CTE, linear 100 - 140 µm/m-°C

@Temperature 20.0 °C
55.6 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Polimersan Plastics POLITEF® (PTFE) with 15% Glass
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
CTE, linear 120 - 140 µm/m-°C

@Temperature 20.0 °C
66.7 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Polimersan Plastics POLITEF® (PTFE)
POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of ..
CTE, linear 100 - 140 µm/m-°C

@Temperature 20.0 °C
55.6 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Polimersan Plastics POLITEF® (PTFE) with 15% Glass
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
CTE, linear 50.0 - 140 µm/m-°C
27.8 - 77.8 µin/in-°F
Average value: 71.1 µm/m-°C Grade Count:25
Overview of materials for PVC, High Impact
This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M..
CTE, linear 18.0 - 140 µm/m-°C
10.0 - 77.8 µin/in-°F
Average value: 63.7 µm/m-°C Grade Count:163
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
CTE, linear 54.0 - 140 µm/m-°C
30.0 - 77.8 µin/in-°F
Average value: 103 µm/m-°C Grade Count:4
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
CTE, linear 120 - 140 µm/m-°C

@Temperature 20.0 °C
66.7 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound  (discontinued **)
Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall..
CTE, linear 120 - 140 µm/m-°C

@Temperature 20.0 °C
66.7 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound  (discontinued **)
Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..
CTE, linear 80.0 - 140 µm/m-°C

@Temperature 20.0 °C
44.4 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
CTE, linear 90.0 - 140 µm/m-°C

@Temperature 30.0 - 300 °C
50.0 - 77.8 µin/in-°F

@Temperature 86.0 - 572 °F
Average value: 113 µm/m-°C Grade Count:2
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min..
CTE, linear 120 - 140 µm/m-°C
66.7 - 77.8 µin/in-°F
Average value: 126 µm/m-°C Grade Count:16
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
CTE, linear 60.0 - 140 µm/m-°C
33.3 - 77.8 µin/in-°F
Average value: 97.5 µm/m-°C Grade Count:4
Overview of materials for Nylon 12, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
CTE, linear 125 - 140 µm/m-°C

@Temperature 23.0 - 100 °C
69.4 - 77.8 µin/in-°F

@Temperature 73.4 - 212 °F
ASTM D696
Manifattura Cattaneo PVDF
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
CTE, linear 110 - 140 µm/m-°C
61.1 - 77.8 µin/in-°F
Master Bond MasterSil 156 Two Part, Low Viscosity Silicone
Description: Master Bond MasterSil 156 is a two component, lower viscosity silicone system for high performance potting, encapsulation and sealing. MasterSil 156 combines high temperature resistance..
CTE, linear 120 - 140 µm/m-°C

@Temperature 20.0 °C
66.7 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Zeus PFA Tubing
PFA, or perfluoroalkoxy, is well recognized for its ability to maintain mechanical integrity in extreme temperatures even when exposed to caustic chemicals. PFA comes in high purity versions that ar..
CTE, linear 120 - 140 µm/m-°C

@Temperature 20.0 °C
66.7 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer  (discontinued **)
Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
CTE, linear 120 - 140 µm/m-°C

@Temperature 20.0 °C
66.7 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer  (discontinued **)
Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO..
CTE, linear 120 - 140 µm/m-°C

@Temperature 20.0 °C
66.7 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer  (discontinued **)
Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
CTE, linear 120 - 140 µm/m-°C

@Temperature 20.0 °C
66.7 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer  (discontinued **)
Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c..
CTE, linear 70.0 - 140 µm/m-°C
38.9 - 77.8 µin/in-°F
Average value: 119 µm/m-°C Grade Count:29
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
CTE, linear 30.0 - 140 µm/m-°C
16.7 - 77.8 µin/in-°F
Average value: 63.7 µm/m-°C Grade Count:20
Overview of materials for Polypropylene, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values..
CTE, linear 140 - 140 µm/m-°C

@Temperature 60.0 - 138 °C
77.8 - 77.8 µin/in-°F

@Temperature 140 - 280 °F
Average value: 140 µm/m-°C Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..