Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimersan Plastics POLITEF® (PTFE) with 15% Glass

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer Polimersan Plastics
Trade Name POLITEF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimersan Plastics POLITEF® (PTFE) with 15% Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical ConductivityIncrease At Corrosion ResistanceIncrease In Deformation Strength Against Load Decrease In Thermal ExpansionHigh Resistance Against AcidsEasiness At Mechanical Processing StretchingResistance Against StrokeIncrease In Thermal Conductivity Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.
Physical Properties Metric English Comments
Specific Gravity 2.10 - 2.30 g/cc
2.10 - 2.30 g/cc
ASTM D1457-18
Deformation 9.8 %
9.8 %
230°C, 1 day, 140 kg/cm^2; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 57 - 62
57 - 62
ASTM D2240
Tensile Strength, Yield 21.6 - 23.5 MPa
3130 - 3410 psi
ASTM D1708
Elongation at Break 290 - 300 %
290 - 300 %
ASTM D1708
Izod Impact, Notched 1.37 J/cm
2.57 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 100 - 140 µm/m-°C

@Temperature 20.0 °C
55.6 - 77.8 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Thermal Conductivity 0.5577 W/m-K
3.864 BTU-in/hr-ft²-°F
ASTM C177
Electrical Properties Metric English Comments
Dielectric Strength 16.0 - 19.0 kV/mm
406 - 483 kV/in
ASTM D149
Descriptive Properties Value Comments
Corrosion 15 - 25 cc-dak/kg-ms
25 - 1000°C
Kinding Temperature 630
°C, ASTM D1929
Users viewing this material also viewed the following: