Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 °C |
5.00 µin/in-°F @Temperature 68.0 °F |
|
Potters Industries Spheriglass® 2530 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 °C |
5.00 µin/in-°F @Temperature 68.0 °F |
|
Potters Industries Spheriglass® 5000 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9294 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9338 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9410 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 30.0 - 300 °C |
5.00 µin/in-°F @Temperature 86.0 - 572 °F |
|
Novum Glass Solid Soda-lime Industrial Series Glass Microspheres Solid soda-lime glass microspheres in colorless powder form. Industrial Series Microspheres are solid glass microspheres (also referred to as soda lime glass beads, glass spheres, or microbeads) us.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | Below glass transition temp; ASTM D696 |
Performance Polymers IPS II PPL-C4270 PEKK (Polyetherketoneketone) Linear 40% Carbon Fiber Reinforced Molding Grade Black pelletsInformation provided by Infinite Polymer System II. |
|||
CTE, linear | 9.00 - 12.0 µm/m-°C @Temperature -40.0 - 125 °C |
5.00 - 6.67 µin/in-°F @Temperature -40.0 - 257 °F |
IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature -40.0 - 149 °C |
5.00 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Duratron® T7130 PAI Polyamide-imide, carbon fiber reinforced, extruded (ASTM Product Data Sheet) |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 30.0 - 300 °C |
5.00 µin/in-°F @Temperature 86.0 - 572 °F |
|
Novum Glass Solid Soda-lime Uniform Series Glass Microspheres Solid soda-lime glass microspheres in colorless powder form. Uniform Series Microspheres are used for controlling a bond line thickness in adhesive bonding. Solid glass microspheres are used in a v.. |
|||
CTE, linear | 9.00 - 36.0 µm/m-°C @Temperature 100 - 200 °C |
5.00 - 20.0 µin/in-°F @Temperature 212 - 392 °F |
Average value: 18.9 µm/m-°C Grade Count:18 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 30.0 - 300 °C |
5.00 µin/in-°F @Temperature 86.0 - 572 °F |
|
Mo-Sci Corporation GL-0191 Soda-Lime Glass Spheres Appearance: Solid soda-lime glass beads with light green color in powder formTypical applications of GL0191 beads include: spacer material for gauge control, coating, filler for plastic, retroreflec.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 30.0 - 300 °C |
5.00 µin/in-°F @Temperature 86.0 - 572 °F |
|
Mo-Sci Corporation GL-0252 Blue Soda-Lime Glass Spheres Appearance: Solid soda-lime glass microspheres with light blue color in powder form.Typical applications of GL-0252 glass microspheres include: spacer for gauge control, thermal expansion reduction .. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1105-0699 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7980 PEEK, with carbon fiber Applications: medical engineeringHigh-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flamm.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 100 °C |
5.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); STA Cold Formable Medium-Strength AlloyFeatures: This binary, age hardening alloy combines the easy formability and weldability of commercially pure titanium with improved mechanical properties, particu.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 100 °C |
5.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 10% Equiaxed Alpha + Annealed This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 10% Equiaxed Alpha + Annealed (705°C/1hr/AC) condition. Other data below are typical of TIMETAL® 6-2-4-6. .. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 100 °C |
5.00 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 6-2-4-6 Titanium Alloy (Ti-6Al-2Sn-4Zr-6Mo), 50% Equiaxed Alpha + STA This entry has UTS, TYS, Elongation, ROA, and fatigue values specific to material in the 50% Equiaxed Alpha + STA (885°C/1hr/AC + 595°C/8hr/AC) condition. Other data below are typical of TIMETAL®.. |
|||
CTE, linear | 9.00 - 36.0 µm/m-°C @Temperature 20.0 - 1000 °C |
5.00 - 20.0 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Goodfellow Potassium Aluminosilicate (Muscovite Mica) Mica is a naturally occurring mineral and as such its exact composition varies between grades, as will its properties. Ruby Mica is the highest grade of Muscovite Mica. The name comes from the Latin.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 600 °C |
5.00 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C373 |
CeramTec 192/193 Titania 192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra.. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | |
CoorsTek StatSafe™ ZDC Static Dissipative Zirconia Specialized StatSafe™ ESD-safe zirconia combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffne.. |
|||
CTE, linear | 9.00 - 10.0 µm/m-°C @Temperature 1000 °C |
5.00 - 5.56 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-B937 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | y direction |
Arlon TC600 Glass, PTFE and Micro-Dispersed Ceramic High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 950 °C |
5.00 µin/in-°F @Temperature 68.0 - 1740 °F |
|
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
CTE, linear | 9.00 µm/m-°C | 5.00 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |
|||
CTE, linear | 9.00 - 162 µm/m-°C | 5.00 - 90.0 µin/in-°F | Average value: 46.3 µm/m-°C Grade Count:23 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 - 1250 °C |
5.00 µin/in-°F @Temperature 68.0 - 2280 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
CTE, linear | 9.00 µm/m-°C @Temperature 20.0 °C |
5.00 µin/in-°F @Temperature 68.0 °F |
Longitudinal; ASTM E228 |
Polystrand ThermoPro™ IE7010 Unitape Unidirectional Polypropylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |