Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 54.0 µm/m-°C @Temperature -18.0 - 38.0 °C |
30.0 µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
Plaskolite Duraplex® 30% I Impact Modified Acrylic Sheet Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc. |
|||
CTE, linear | 54.0 µm/m-°C @Temperature -18.0 - 38.0 °C |
30.0 µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
Plaskolite PETG Mirror Sheet Versatile fabrication properties with good impact strength, good design flexibility, and speed of fabrication.Data provided by the manufacturer, Plaskolite, Inc. |
|||
CTE, linear | 54.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E831 |
Quadrant EPP Fluorosint® MT-01 Proprietary fluoropolymer reinforced with carbon fibers and organometallic fillers( ASTM Product Data Sheet) |
|||
CTE, linear | 54.0 µm/m-°C @Temperature -34.4 - -1.11 °C |
30.0 µin/in-°F @Temperature -30.0 - 30.0 °F |
ASTM D696 |
Plaskolite Optix® DA Digital Acrylic Sheet Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup.. |
|||
CTE, linear | 54.0 - 160 µm/m-°C | 30.0 - 88.9 µin/in-°F | Average value: 105 µm/m-°C Grade Count:7 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 54.0 - 340 µm/m-°C | 30.0 - 189 µin/in-°F | Average value: 233 µm/m-°C Grade Count:49 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
CTE, linear | 54.0 µm/m-°C @Temperature -40.0 - 176 °C |
30.0 µin/in-°F @Temperature -40.0 - 349 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
CTE, linear | 54.0 µm/m-°C @Temperature -18.0 - 38.0 °C |
30.0 µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
Plaskolite Optix® PL-30 Acrylic Resin
(discontinued **) Injection molding and extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line with exceptional mold release.Data provided by the manufacturer, Plaskolite, Inc. |
|||
CTE, linear | 54.0 µm/m-°C @Temperature -18.0 - 38.0 °C |
30.0 µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
Plaskolite Optix® PL-52 Acrylic Resin
(discontinued **) Injection/extrusion pellets. High heat resistance/medium flow.Data provided by the manufacturer, Plaskolite, Inc. |
|||
CTE, linear | 54.0 - 62.0 µm/m-°C | 30.0 - 34.4 µin/in-°F | Average value: 57.2 µm/m-°C Grade Count:8 |
Overview of materials for PVC, Powder This property data is a summary of similar materials in the MatWeb database for the category "PVC, Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
CTE, linear | 54.0 - 55.0 µm/m-°C @Temperature 73.0 - 200 °C |
30.0 - 30.6 µin/in-°F @Temperature 163 - 392 °F |
Average value: 54.5 µm/m-°C Grade Count:2 |
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
CTE, linear | 54.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E831 |
Quadrant EPP Fluorosint® MT-01 Enhanced PTFE (ASTM Product Data Sheet)
(Unverified Data**) |
|||
CTE, linear | 54.0 - 144 µm/m-°C @Temperature 25.6 - 204 °C |
30.0 - 80.0 µin/in-°F @Temperature 78.0 - 400 °F |
ASTM D696 |
Technetics Group Texolon™ 9406 PTFE
(Unverified Data**) General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel.. |
|||
CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | Average value: 54.0 µm/m-°C Grade Count:3 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 54.0 - 144 µm/m-°C @Temperature 25.6 - 204 °C |
30.0 - 80.0 µin/in-°F @Temperature 78.0 - 400 °F |
ASTM D696 |
Garlock 9405 PTFE Rubber Sheet, 25% Glass Filled Premium Grade 25% Glass-filled Skived PTFE SheetInformation provided by Garlock Rubber Technologies |
|||
CTE, linear | 54.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
30.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
LyondellBasell Astryn BB73F Polypropylene Copolymer, Mineral Filled Key Features: high melt flow, high modulus, UV-stabilized, mineral-filled, high rigidity, good impact strength, good dimensional stability, good scratch and mar resistance, excellent processability,.. |
|||
CTE, linear | 54.0 µm/m-°C @Temperature 20.0 °C |
30.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® High Performance Extruded PEI Film Description: PEI = polyetherimide. Used Primarily for Electrical/Electronics ApplicationsInformation provided by Saint Gobain Performance Products. |
|||
CTE, linear | 54.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
30.0 µin/in-°F @Temperature -22.0 - 176 °F |
Borealis Method |
Borealis Daplen™ EF341AE Polypropylene TPO Compound Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | |
Unifrax Fiberfrax® Rigidizer™ Inorganic Liquid Hardener Rigidizer™ and Rigidizer™ W, inorganic liquid hardeners, have a temperature grade rating of 1260°C (2300°F). They are generally used to increase the durability and surface erosion resistance of.. |
|||
CTE, linear | 54.0 µm/m-°C @Temperature 40.0 - 130 °C |
30.0 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 1530 Polyester, Briquette, Transfer Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
CTE, linear | 54.0 µm/m-°C @Temperature 40.0 - 130 °C |
30.0 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 7080 Phenolic, Nodular, Compression Molded PLENCO 07080 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties along with outstanding resistance to cracking and degradation from soap and de.. |
|||
CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | |
Hexcel® HexPly® F593 Epoxy Resin HexPly® F593 is a modified 350°F (177°C) curing epoxy system with very low flow for carbon fabric and tape applications that provides excellent laminate and honeycomb sandwich properties. As a lo.. |
|||
CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® 301-1 Optical Grade Epoxy Material Description: A two component, room temperature curing, optical grade epoxy, designed for optics, medical, and opto-electronic packaging of semiconductor devices, components, and electronics.. |
|||
CTE, linear | 54.0 µm/m-°C @Temperature 20.0 °C |
30.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermylene® P6-10FG-Y950 10% Glass Fiber Reinforced, Lubricated Information provided by Asahi Thermofil |
|||
CTE, linear | 54.0 µm/m-°C @Temperature 20.0 °C |
30.0 µin/in-°F @Temperature 68.0 °F |
|
Aremco Aremco-Bond™ 657 High Performance Epoxide Stainless Steel-Filled, High Corrosion Resistance. |
|||
CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | |
Unifrax Fiberfrax® QF-150™ Coating Cement Fiberfrax QF-180™, QF-180™ Blue, and QF-150™ coating cements provide a range of consistencies for brush, spray, and trowel-on application. These coatings have 1260°C (2300°F) temperature grade.. |
|||
CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | |
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad.. |
|||
CTE, linear | 54.0 - 90.0 µm/m-°C | 30.0 - 50.0 µin/in-°F | Average value: 72.0 µm/m-°C Grade Count:5 |
Overview of materials for Acrylic, Impact Modified Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 54.0 µm/m-°C | 30.0 µin/in-°F | |
Unifrax Fiberfrax® Rigidizer™ W Inorganic Liquid Hardener Rigidizer™ and Rigidizer™ W, inorganic liquid hardeners, have a temperature grade rating of 1260°C (2300°F). They are generally used to increase the durability and surface erosion resistance of.. |