Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 60.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 140 °F |
|
Omnia Plastica Akulon® POM h Acetal Homopolymer The general features of homopolymer acetalic resin are similar to those of copolymer POM c, except that service temperature (under load) is slightly higher but resistance to hydrolysis and strong al.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 60.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 140 °F |
|
Omnia Plastica Arnite Omnialite POM c Acetal Copolymer Polyoxymethylene, commonly called Acetal, is a crystalline polymer obtained from the polymerisation of formaldehyde. Discovered fairly recently (1960), it has enjoyed rapid growth and large acceptan.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
DIN 53752 |
Polycasa XT 610 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Celanex® 2008 PBT
(Unverified Data**) Celanex 2008 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Ultrahigh melt flowInfor.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Celcon® M140-L1 POM, Tribological
(Unverified Data**) Celcon® M140-L1 is a general purpose acetal copolymer material with a slightly lower viscosity for improved flow in molding that has been modified to reduce or eliminate noise (squeak) when wearing.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Celcon® UV270Z POM, UV Resistant
(Unverified Data**) Celcon® UV270Z is a nominal 27 melt flow rate acetal copolymer which has been specially stabilized to prevent discoloration and deterioration of mechanical properties from ultraviolet light exposur.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® AM90S Plus POM, Specialty
(Unverified Data**) Hostaform® acetal copolymer grade AM90S Plus is a standard melt viscosity acetal copolymer material containing an antimicrobial ingredient. AM90S Plus reaches maximum efficacy more rapidly than st.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® C 2521 POM
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMStiff-flowing grade for injection molding and extrusionInformation provided by Celanese |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® C 9021 M POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, with molybdenum disulphide modifiedInformation provided by Celanese |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® MT24U01 POM, Medical Technology
(Unverified Data**) Hostaform® MT24U01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform® MT24U01 is a low melt viscosity for fast cycli.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® MT8U01 POM, Medical Technology
(Unverified Data**) Hostaform® acetal copolymer grade MT8U01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform® MT8U01 is an injection m.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
CTE, linear | 110 - 130 µm/m-°C @Temperature 20.0 °C |
61.1 - 72.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | DIN 52328 |
Isoflon PA 12 Polyamide 12 General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ASTM E831 |
Lucite International Diakon® ST35G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond 2162D Color Coded Smooth Paste Epoxy Adhesive TRA-BOND 2162D epoxy system is color-coded for easy mixing and handling as a smooth paste, and it develops strong bonds to most materials including metals, glass, ceramics, leather, wood, concrete a.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® SX-35 Acetal Co-polymer (POM), Flexible, Lower noise DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Bayflex® XGT-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-2 |
Celanese Celanex® 2403 MT Unreinforced PBT with Improved Crystallization Speed Description: Celanex 2403 MT Natural is an unreinforced PBT with improved crystallization speed and faster cycle times that complies with the requirements of the FDA and is listed in the Drug Master.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
CENTROPLAST CENTRODAL LF Polyoxymethylene conductive This material is electrically conductive, with high mechanical strength and dimensional stability. Applications include structural components in potentially explosive areas, components for divertin.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Celcon® M270™ POM
(Unverified Data**) Celcon® acetal copolymer grade M270™ is a lower molecular weight, high - flow grade designed for superior moldability in multi-cavity, intricate or hard to fill molds applications.General purpose,.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Celcon® M90-45XAP® POM, Specialty
(Unverified Data**) Celcon® acetal copolymer grade M90-45XAP® is a UV resistant, low emission version, medium viscosity polymer providing optimum performance in general purpose injection molding primarily for the in.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® S 9363 POM, Impact Modified
(Unverified Data**) Hostaform® acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform® S 9363 provides good impact strength while improving modulus and weld line strength o.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® EB-08 Acetal Co-polymer (POM), Conductive, Antistatic DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |