Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 110 µm/m-°C @Temperature 25.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 77.0 - 131 °F |
ASTM E831 |
Shell Carilon® D26VM100 Polyketone, High-Flow Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26VM100 is a high-flow injection molding grade with mechanical properties which classify it as an .. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Celcon® UV270Z POM, UV Resistant
(Unverified Data**) Celcon® UV270Z is a nominal 27 melt flow rate acetal copolymer which has been specially stabilized to prevent discoloration and deterioration of mechanical properties from ultraviolet light exposur.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® C 9021 LS POM, UV Resistant
(Unverified Data**) POM copolymerUV resistantInformation provided by Celanese |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® C 9021 M POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, with molybdenum disulphide modifiedInformation provided by Celanese |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® C 9021 S1 POM, Tribological
(Unverified Data**) modified with silicon oilInformation provided by Celanese |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® MT8F02 POM, Medical Technology
(Unverified Data**) Hostaform® acetal copolymer grade MT8F02 is a special grade developed for medical industry applications containing low residual monomers. Hostaform® MT8F02 is a standard flow high level polytetra.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Hostaform® MT8U01 POM, Medical Technology
(Unverified Data**) Hostaform® acetal copolymer grade MT8U01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform® MT8U01 is an injection m.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
CTE, linear | 110 - 130 µm/m-°C | 61.1 - 72.2 µin/in-°F | |
Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System Master Bond Polymer System EP21TDC-4 is a two component, flexible epoxy resin system for high performance bonding, sealing and coating. It is formulated to cure at ambient temperatures or more quick.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® M450-44/M450S Acetal Co-polymer (POM), Standard, Super high flow, High cycle DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
|
Loctite® 3873 1 component acrylic High Conductivity Flexible Adhesive Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 307A4000015 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 380A3V32818 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Bayflex® 110-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
silicone property; ASTM E 831 |
Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359-2 |
Celanese Celanex® 2403 MT Unreinforced PBT with Improved Crystallization Speed Description: Celanex 2403 MT Natural is an unreinforced PBT with improved crystallization speed and faster cycle times that complies with the requirements of the FDA and is listed in the Drug Master.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® M140-44/M140S Acetal Co-polymer (POM), Standard, High flow DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® NW-02 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | ISO 11359-2 |
Celanese Celanex® 1400FC PBT
(Unverified Data**) Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a.. |
|||
CTE, linear | 110 µm/m-°C @Temperature -30.0 - 100 °C |
61.1 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hifax™ CA186 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent paintability and paint durability, good processabi.. |
|||
CTE, linear | 110 - 130 µm/m-°C | 61.1 - 72.2 µin/in-°F | ASTM D696 |
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | Average above Tg; ISO 11359 |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |