Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 145 °C | 293 °F | STN EN 11357-1 |
Plastcom PLASTALEN® EH 91 N Polyethylene HDPE regrind for injection molding. General use in all industry branches. Delivered in blue ( approx. RAL 5015) mode.Information Provided by Plastcom spol. s r.o. |
|||
Melting Point | 145 °C | 293 °F | |
Plastcom SLOVALEN PC 11 N PP, imp. strength Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Melting Point | 145 °C | 293 °F | |
Plastcom SLOVALEN PC 59 GF 30 PP, 30% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains themodifier of mechanical properties.Increased strength in comparison with unfilled PP. A.. |
|||
Melting Point | 145 °C | 293 °F | |
Plastcom SLOVALEN PC 78 FRT 5 PP, glass fibre, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfilled.. |
|||
Melting Point | 145 °C | 293 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant FeaturesModified homopolymer PP for injection moulding, contains the modifier of mechanical properties and non halogen and free phosphor flame retardant. Increased strength in comparison with unfil.. |
|||
Melting Point | 145 - 160 °C | 293 - 320 °F | Peak; ASTM D3418 |
NatureWorks® Ingeo™ 2003D General Purpose Transparent Extrusion Grade Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed fo.. |
|||
Melting Point | 145 - 160 °C | 293 - 320 °F | Peak; ASTM D3418 |
NatureWorks® Ingeo™ 3052D Lubricated, High Flow Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. It is designed for injection molding applications where the requirements are clarity with heat def.. |
|||
Melting Point | 145 - 160 °C | 293 - 320 °F | Peak; ASTM D3418 |
NatureWorks® Ingeo™ 8052D Foam Grade Biopolymer Ingeo 8052D can be converted into an expanded foam sheet with use temperatures up to 77°F (25°C). This foam is lightweight, strong and suitable for packaging fresh meat and vegetables. In order to.. |
|||
Melting Point | 145 °C | 293 °F | STN EN 11357-1 |
Plastcom SLOVALEN PC 99 GF 30/1M Polypropylene reinforced with glass fiber, improved flowing Modified copolymer PP for injection molding, reinforced with 30% glass fiber, improved flowing. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Informatio.. |
|||
Melting Point | 145 °C | 293 °F | Flow temperature, ASTM D569 |
Rotuba M Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Melting Point | 145 °C | 293 °F | DSC second heating; ASTM D3418 |
Reliance Industries Repol T100MK Polypropylene REPOL Polypropylene T100MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melting Point | 145 - 160 °C | 293 - 320 °F | Huntsman/TMA |
Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade IROGRAN A 85 E 4993 FCM is a thermoplastic polyester polyurethane for melt calendaring. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a specially.. |
|||
Melting Point | 145 - 156 °C | 293 - 313 °F | TMA Melt Range, 25 mil film |
Huntsman IROGRAN® A 85 P 4394 UV TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
Melting Point | 145 - 160 °C | 293 - 320 °F | ISO 3146-C |
FKuR Kunststoff Bio-Flex® F 2201 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melting Point | 145 °C | 293 °F | Eutectic |
Indium Corp. Indalloy® 181 Sn-Pb-Cd Solder Alloy Good general purpose solder in the medium temperature range. Maintains its creep strength well. Not applicable against gold.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 145 °C | 293 °F | ASTM D2117 |
Lushan PF-3 Adhesive Resin for Coextruded Multi-layer Barrier Packaging Film Adhesive resin Lushan series for multi-layer barrier food packaging film has durable bonding properties when adheres to Polarity materials, such as PE, PP and PA, EVOH, etc. Adhesive resin Lushan se.. |
|||
Melting Point | 145 - 160 °C | 293 - 320 °F | |
Indium Corp. Indalloy 94 Lead-Tin-Cadmium Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 145 °C | 293 °F | ASTM D3418 |
UBE P7115U Electronic Grade Nylon Copolymer Powder Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Melting Point | 145 °C | 293 °F | DSC |
Total PPR 6827MZ Polypropylene, Random Copolymer - High Flow Clarified - for Injection Molding Clarity. TOTAL Polypropylene 6827MZ exhibits superior clarity and produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.Antistat. 6827MZ contains an a.. |
|||
Melting Point | 145 °C | 293 °F | DSC |
Total PPR 7425 Polypropylene, Injection Molding Grade Random copolymer for injection moldingClarity - FINA 7425, a random copolymer, exhibits excellent clarity when molded in polished molds.Impact - FINA 7425 produced molded parts with measurably impro.. |
|||
Melting Point | 145 °C | 293 °F | Kofler |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |
|||
Melting Point | 145 °C | 293 °F | ASTM D3418 |
UBE 7115U Nylon 6/12 Copolymer Description: UBESTA Nylon 12 CopolymerInformation provided by UBE. |
|||
Melting Point | 145 °C | 293 °F | ISO 3146 |
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld.. |
|||
Melting Point | 145 - 155 °C | 293 - 311 °F | DSC |
EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 145 - 155 °C | 293 - 311 °F | DSC |
EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | <= 145 °C | <= 293 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ MV 02528EH2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 02528EH2 is a copolymer of ethylene and vinyl acetate.Availability: Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent: Yes A.. |
|||
Melting Point | 145 °C | 293 °F | |
BASF Novolen® 3200 H Polypropylene Blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 145 °C | 293 °F | Kofler |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |
|||
Melting Point | 145 - 168 °C | 293 - 334 °F | Average value: 161 °C Grade Count:8 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |