Material Notes:
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
Melt Flow 0.50 g/10 min

@Load 0.325 kg,
Temperature 270 °C
0.50 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
Elongation at Break 200 %
200 %
Flexural Modulus 1.30 GPa
189 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
Charpy Impact, Notched 1.00 J/cm²

@Temperature -20.0 °C
4.76 ft-lb/in²

@Temperature -4.00 °F
8.50 J/cm²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 145 °C
293 °F
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
Vicat Softening Point 150 °C
302 °F
B
Processing Properties Metric English Comments
Melt Temperature 200 - 220 °C
392 - 428 °F