Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 145 - 156 °C | 293 - 313 °F | TMA Melt Range, 25 mil film |
Huntsman IROGRAN® A 85 P 4394 UV TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |