Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ MV 02528EH2 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ MV 02528EH2 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: UL 02528EH2 is a copolymer of ethylene and vinyl acetate.Availability: Asia Pacific and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent: Yes Applications: Hot Melt AdhesivesViscosity Modifier Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
ExxonMobil method
Viscosity 3100 cP

@Temperature 190 °C
3100 cP

@Temperature 374 °F
Melt
Vinyl Acetate Content 27.5 %
27.5 %
ExxonMobil method
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.52 MPa
220 psi
(20 in/min), Molded Properties; ASTM D638
Elongation at Break 140 %
140 %
(20 in/min), Molded Properties; ASTM D638
Tensile Modulus 0.00827 GPa
1.20 ksi
(0.2 in/min), Molded Properties; ASTM D638
Thermal Properties Metric English Comments
Melting Point <= 145 °C
<= 293 °F
Peak Melting Point; ExxonMobil method
Users viewing this material also viewed the following: