Material Notes:
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains themodifier of mechanical properties.Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased strength, toughness, modulus in tension due to themodification. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
Linear Mold Shrinkage 0.0058 cm/cm
0.0058 in/in
Linear Mold Shrinkage, Transverse 0.0127 cm/cm
0.0127 in/in
Melt Flow 5.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
5.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
Elongation at Break 4.0 %
4.0 %
Tensile Modulus 5.40 GPa
783 ksi
Flexural Strength 105 MPa
15200 psi
Flexural Modulus 4.70 GPa
682 ksi
Charpy Impact Unnotched 4.50 J/cm²

@Temperature -20.0 °C
21.4 ft-lb/in²

@Temperature -4.00 °F
5.50 J/cm²

@Temperature 23.0 °C
26.2 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 145 °C
293 °F
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Vicat Softening Point 155 °C
311 °F
B
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi
Users viewing this material also viewed the following: