Total PPR 6827MZ Polypropylene, Random Copolymer - High Flow Clarified - for Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPR
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPR 6827MZ Polypropylene, Random Copolymer - High Flow Clarified - for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clarity. TOTAL Polypropylene 6827MZ exhibits superior clarity and produces molded parts with improved impact compared with parts molded from homopolymer polypropylene.Antistat. 6827MZ contains an antistat to help protect molded parts from dust accumulation.Easy Flow. 6827MZ exhibits exceptionally easy flow characteristics.FDA - 6523WZ complies with all applicable FDA and USDA regulations and may be used under these provisions for food contact and packaging.Recommended Applications. - 6827MZ is recommended for injection molding housewares, cassette cases and other items calling for a combination of good impact and superior clarity.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238, L
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Tensile Modulus 1.17 GPa
170 ksi
ASTM D638
Flexural Modulus 1.03 GPa
149 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256A
Impact Test 18.7 J

@Thickness 3.17 mm
13.8 ft-lb

@Thickness 0.125 in
Drop Impact; API
Thermal Properties Metric English Comments
Melting Point 145 °C
293 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
ASTM D648