Physical Properties Metric English Comments
Density 8.36 g/cc
0.302 lb/in³
Thermal Properties Metric English Comments
Melting Point 145 - 160 °C
293 - 320 °F
Solidus 145 °C
293 °F
Liquidus 160 °C
320 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 25 %
25 %
Lead, Pb 25 %
25 %
Tin, Sn 50 %
50 %