Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. Indalloy® 181 Sn-Pb-Cd Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 181 Sn-Pb-Cd Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good general purpose solder in the medium temperature range. Maintains its creep strength well. Not applicable against gold.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 8.45 g/cc
0.305 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 43.2 MPa
6270 psi
Thermal Properties Metric English Comments
CTE, linear 24.0 µm/m-°C

@Temperature 20.0 °C
13.3 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 35.0 W/m-K

@Temperature 85.0 °C
243 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 145 °C
293 °F
Eutectic
Solidus 145 °C
293 °F
Liquidus 145 °C
293 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 18.2 %
18.2 %
Lead, Pb 30.6 %
30.6 %
Tin, Sn 51.2 %
51.2 %
Users viewing this material also viewed the following: