Austin Novel Materials Texalan® 670A Polyester and Polyether based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Austin Novel Materials
Trade Name Texalan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Austin Novel Materials Texalan® 670A Polyester and Polyether based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Physical Properties Metric English Comments
Density 1.12 - 1.16 g/cc
0.0405 - 0.0419 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 67 - 73
67 - 73
ISO 7619
Tensile Strength >= 21.0 MPa
>= 3050 psi
ISO 37
Tensile Stress >= 2.50 MPa

@Strain 100 %
>= 363 psi

@Strain 100 %
ISO 37
>= 4.00 MPa

@Strain 300 %
>= 580 psi

@Strain 300 %
ISO 37
Elongation at Yield >= 700 %
>= 700 %
ISO 37
Tear Strength >= 45.0 kN/m
>= 257 pli
ISO 34
K Factor (Wear Factor) <= 70
<= 70
[mm<sup>3</sup>]; ISO 4649
Compression Set <= 32 %

@Temperature 70.0 °C
<= 32 %

@Temperature 158 °F
ISO 815