Lord Adhesives Versilok® 262B / 254 Acrylic Adhesive

Category Polymer , Adhesive
Manufacturer Lord Adhesives
Trade Name Versilok®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Versilok® 262B / 254 Acrylic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LORD Versilok® 262B/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare aluminum, and cold rolled steel. Versilok 262B/254 adhesive can be either room temperature cured or heat cured for faster processing.Versilok 262B/254 adhesive contains an odor suppressant. Versilok 262B/254 adhesive is recommended for applications where glass beads are not desired. Versilok 262B/254 adhesive is approved by BMW (GS97028-12).All information provided by Lord.
Physical Properties Metric English Comments
Density 1.10 - 1.16 g/cc
0.0397 - 0.0419 lb/in³
262B Resin
1.39 - 1.46 g/cc
0.0502 - 0.0527 lb/in³
254 Hardener
Brookfield Viscosity 40000 - 300000 cP

@Temperature 25.0 °C
40000 - 300000 cP

@Temperature 77.0 °F
254 Hardener; HAT-TD @ 5rpm
195000 - 435000 cP

@Temperature 25.0 °C
195000 - 435000 cP

@Temperature 77.0 °F
262B Resin; HAT-TD @ 5rpm
Mechanical Properties Metric English Comments
Impact Test >= 10.2 J
>= 7.50 ft-lb
GM 9751P
Peel Strength >= 5.26 kN/m
>= 30.0 pli
ASTM D1876
Thermal Properties Metric English Comments
Flash Point >= 93.0 °C
>= 199 °F
262B Resin; Closed Cup
>= 93.0 °C
>= 199 °F
254 Hardener; Closed Cup
Descriptive Properties Value Comments
Appearance Gray
254 Hardener
White/Light Green
262B Resin
Consistency Paste
262B Resin
Paste
254 Hardener
Press Flow (sec) 15-55
20g, 80psi @ 25ºC; orifice #1, 0.052"
20-60
20g, 80psi @ 25ºC; orifice #1, 0.052"