Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Cast
Manufacturer Ensinger
Trade Name TECAST VEKTON™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tecast® 6PA Black is a black cast nylon that is more UV resistant than natural nylon 6.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of good mechanical properties, excellent bearing and wear characteristics, and the large-size capabilities of the casting process. Its fatigue resistance, noise damping ability, corrosion resistance, and light weight make Tecast ideal for metal replacement applications, such as bearings, gears, sheaves, and sprockets. At one-eight the weight of bronze, Tecast is easier to handle and maintain than metals such as iron, aluminum, brass, and bronze, which it typically replaces in industrial wear applications. Other materials that Tecast commonly replaces because of its superior performance are laminated phenolics, elastomers, and wood. Tecast has excellent wear and abrasion resistance, resulting in extended component life and lower maintenance cost. Its formulations are readily available in rod, plate, and tube. Nonstandard shapes, such as rings, discs, and blocks can be economically produced in small quantities with short lead times. Custom parts can be cast-size or near-net-shape with relatively inexpensive tooling. General Tecast® Application Information: Its unique combination of strength, wear resistance, toughness, machinability, and corrosion resistance make Tecast cast nylon ideal for bearings, thrust washers, bushings, wear pads, sheaves, rollers, gears, sprockets, and wheels. Tecast is commonly used in construction equipment, material handling systems, amusement park rides, pulp and paper processing equipment, steel mills and industrial equipment. Information supplied by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.15 - 1.16 g/cc
0.0416 - 0.0419 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
at 24 hours; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D638
Flexural Strength 86.2 MPa
12500 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.26
0.26
40 psi, 50 fpm; ASTM D3702
K (wear) Factor 403 x 10-8 mm³/N-M
200 x 10-10 in³-min/ft-lb-hr
40 psi, 50 fpm; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.67 J/g-°C
0.400 BTU/lb-°F
Thermal Conductivity 0.241 W/m-K
1.67 BTU-in/hr-ft²-°F
Melting Point 220 °C
428 °F
ASTM D2133
Maximum Service Temperature, Air 93.3 °C
200 °F
Long Term; ASTM UL746B
149 °C
300 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 188 °C
370 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C
200 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Constant 3.7

@Frequency 60 Hz
3.7

@Frequency 60 Hz
ASTM D150
3.7

@Frequency 60 Hz
3.7

@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 19.7 kV/mm
500 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 60 Hz
0.0020

@Frequency 60 Hz
ASTM D150