Polymer Property : Density = 1.15 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
STN 64 0111
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Density 1.15 g/cc
0.0415 lb/in³
NCMT Method
NCMT NanoPAC™ HG537 High Performance Polypropylene Nanocomposite
Applications: Household Industry Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
SABIC Innovative Plastics Cycoloy® C3100 PC+ABS (Europe-Africa-Middle East)
C3100 is blow moulding/extrusion grade offering low temperature ductility, high heat resistance and high meltstrength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Nilit FRIANYL A63 M2 Nylon 6.6 for injection molding, 2% molybdenum disulphide lubricated
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
SABIC Innovative Plastics Cycoloy® FXC810AL PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810AL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Alpine White colour effects. The colour package may effect performance.This data was..
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
SABIC Innovative Plastics GELOY XP4034 ASA+PC (Europe-Africa-Middle East)
GELOY XP4034 is a high heat modified ASA+PC alloy. It is a weatherable, injection mouldable product which is available in a wide range of colours. The product is recommended for automotive unpainted..
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific)
Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region.
Density 1.15 - 1.38 g/cc
0.0415 - 0.0499 lb/in³
Average value: 1.20 g/cc Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Density 1.15 - 1.19 g/cc
0.0415 - 0.0430 lb/in³
Average value: 1.18 g/cc Grade Count:11
Overview of materials for Acrylic, High Flow, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app..
Density 1.15 g/cc
0.0415 lb/in³
DIN EN ISO 1183-1
Kraiburg TPE THERMOLAST® K TC4PAZ Thermoplastic Elastomer, Adhesion to PA
The AD/PA Series is recommended for applications with excellent adhesion to PA. The compounds are available in natural and black colors. Typical applications: Cable clipsFunction and design elements..
Density 1.15 g/cc
0.0415 lb/in³
DIN EN ISO 1183-1
Kraiburg TPE THERMOLAST® K TC6NYZ Thermoplastic Elastomer, Adhesion to PA
The AD/PA/AP Series is recommended for applications with excellent adhesion to PA. The compounds are available in natural and black colors. Typical applications: Cable clipsFunction and design eleme..
Density 1.15 g/cc
0.0415 lb/in³
DIN 53479
Kraiburg TPE THERMOLAST® K TP5CCN Natural Cable Extrusion TPE
Natural compound for cable extrusionSubstitute for PVC-PExtremely flexible materialFlexible in low temperaturesColoring in any shadeTypical Applications: Transmission cablesLoudspeaker cablesConnect..
Density 1.15 g/cc
0.0415 lb/in³
DIN 53479
Kraiburg TPE THERMOLAST® K TP6CCN Natural Cable Extrusion TPE
Natural compound for cable extrusionSubstitute for PVC-PExtremely flexible materialFlexible in low temperaturesColoring in any shadeTypical Applications: Transmission cablesLoudspeaker cablesConnect..
Density 1.15 g/cc
0.0415 lb/in³
DIN 53479
Kraiburg TPE THERMOLAST® K TC7AGZ Black Sealing TPE
Natural compound for sealing applicationsSeals under static and dynamic loadTypical Applications: Applications in automotive and electric industries with high requirements to compression set (e.g. s..
Density 1.15 g/cc
0.0415 lb/in³
ISO R 1183
Schwartz Technical Plastics OPTAMID® Cast Polyamide 6, Conditioned
Application: deflection rope sheaves for elevatorsInformation provided by Schwartz Technical Plastics GmbH
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Techmer ES HiFill FR® HIPS 1000 FR-E
Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc.
Density 1.15 g/cc
0.0415 lb/in³
Trelleborg Emerson & Cuming Eccobond® D 275 One-Component Fast Cure Epoxy Adhesive
Emerson & Cuming D 275 Eccobond® One-Component Fast Cure Epoxy AdhesiveSemi-rigid, high strength, fast curing, pourable, epoxy structural adhesive. Good peel strength (12 pli), Recommended for bond..
Density 1.15 g/cc
0.0415 lb/in³
ASTM D 792
Cossa Polimeri ESTADIENE 0417 GIF Acrylonitrile Butadiene Styrene, 17% Glass Filled
ABS with 17% glass fiber reinforcementGood thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
BASF Elastollan® C-70AW Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen..
Density 1.15 g/cc
0.0415 lb/in³
BASF N-Formylmorphonline
Formula: C5H9NO2CAS: 4394-85-8Description: N-Formylmorpholine is a colorless to yellowish solid or liquid that is odorless.Synonyms: 4-Morpholinecarbaldehyde, Formylmorpholine, NFMApplications: Inte..
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Ashley Polymers Ashlene® 264-15 PPO, 15% Glass Reinforced
A general purpose, 15% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
CENTROPLAST CENTROMID 6 G Polyamide 6 Cast
This material has good machinability and can be bonded or welded. Its applications include sliding bearings, hammerheads, and toothed gears.Information provided by CENTROPLAST Engineering Plastics ..
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Polykemi AB POLYelast TPE ZS606 Thermoplastic Elastomer, SEBS/SBS-based
Information provided by Polykemi AB
Density 1.15 g/cc
0.0415 lb/in³
DIN EN ISO 1183-1:2004
Kraiburg TPE THERMOLAST® K TC3PAN Thermoplastic Elastomer, Adhesion to PA  (Unverified Data**)
Typical Markets / Application Sectors:Electrical ToolsAutomotive InteriorAutomotive UndercarApplication Examples:HandlesSealsDesign and functional elementsVibration damping elementsAir inlet pipingS..
Density 1.15 g/cc
0.0415 lb/in³
DIN EN ISO 1183-1:2004
Kraiburg TPE THERMOLAST® K TC8PAZ Thermoplastic Elastomer, Adhesion to PA  (Unverified Data**)
Typical Markets / Application Sectors:Electrical ToolsAutomotive InteriorAutomotive UndercarApplication Examples:HandlesSealsDesign and functional elementsVibration damping elementsAir inlet pipingS..
Density 1.15 g/cc
0.0415 lb/in³
Latex
DuPont Performance Polymers Neoprene 400 Polychloroprene  (discontinued **)
Main feature: High modulus and ozone resistance. Principal uses include: Bonded fibers, Coatings, Treated paper, Adhesives (Bonded Batts, Lamination).Solids content: 50%. Initial pH: 12.5. Surfac..
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Techmer ES HiFill® TPX-HTN-01043 A
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: High Temperature Strength, Impact Modified and LubricatedUL File Number: E157318Information provided by TP C..