Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D792-91
Multibase Multi-Pro® 0505 RC Black 5.2% Glass Filled Polypropylene
This product was specially designed for one customer's glass filled polypropylene application.Data provided by Multibase.
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 6348K (486F3) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
Petromont 2001 High Density Polyethylene Resin
Petromont HDPE 2001 is a high-density polyethylene copolymer resin produced using the UNIPOL ® Process. This resin has been designed specifically for film for various applications such as notion an..
Density 0.948 g/cc
0.0342 lb/in³
Exxon Method
ExxonMobil Optema® TC-221 Ethylene Methyl Acrylate for Compounding  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.27% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used for making alloys, blends, and compounds, or be injection molded where..
Density 0.948 g/cc
0.0342 lb/in³
ASTM D4883
ExxonMobil HD 6605.29 Injection Molding Resin  (discontinued **)
HD 6605 is a narrow molecular weight hexene copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance. Ideally suited for ..
Density 0.947 g/cc
0.0342 lb/in³
ASTM D792
NOVA Chemicals Sclair® 8504 BK, 8504 GBK MDPE Rotational Molding Resin  (discontinued **)
Features: Low melt index, excellent ESCR, high toughness at low temperatures.Applications: Large chemical storage tanks.Data provided by the manufacturer.
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
LyondellBasell Alathon® ETP H4745 High Density Polyethylene
ApplicationsALATHON H 4745 is a new, multi-purpose, high-flow resin featuring enhanced cold temperature impact performance, enhanced processability and thermal stability for fast cycling and exhibit..
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
LyondellBasell Alathon® H4620 High Density Polyethylene, Injection Molding Grade
Alathon H4620 is a medium-flow resin that exhibits good cold temperature impact performance, enhanced processing and thermal stability. Typical applications are thinner-walled parts that require che..
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
LyondellBasell Alathon® M4612 High Density Polyethylene
ApplicationsALATHON M 4612 is a copolymer that provides outstanding ESCR and low temperature impact strength. Typical applications include food containers, seat hinges, tube headers.Regulatory Stat..
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
LyondellBasell Alathon® M4661 High Density Polyethylene
ApplicationsALATHON M 4661, formerly known as LYHD 060, exhibits excellent impact, warp and environmental stress crack resistance. Typical applications are closures, institutional seating and consum..
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade
ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a..
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
ICO Polymers ICORENEâ„¢ 150-1050 HDPE Rotational Molding Resin
Description: ICORENE 150-1050 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is..
Density 0.948 g/cc
0.0342 lb/in³
ASTM D4883
Ineos TC46-25 HDPE
TC46-25 is a natural high density polyethylene copolymer designed specifically for telecommunications ducting to meet or exceed the material requirements in ASTM F2160, UL 651B and MEMA TC-7. TC46-..
Density 0.947 g/cc
0.0342 lb/in³
ASTM D4883
Ineos K44-11-128 HDPE
Ineos K44-11-128 is a high molecular weight, high density polyethylene copolymer intended for large part blow molding where the finished product demands good physical performance and low color. Thi..
Density 0.948 - 0.954 g/cc
0.0342 - 0.0345 lb/in³
ASTM D792-98
Ipiranga Petrochem GM 5250 OC HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Density 0.947 g/cc
0.0342 lb/in³
ASTM D792
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Density 0.948 g/cc
0.0342 lb/in³
15.5°C/4°C
Solvay AMGARD® DBBP Phosphorus Derivative
Identification: DIBUTYL BUTYL PHOSPHONATECAS: 78 – 46 – 6Molecular formula: C12H27O3PAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: Organophosphorous comp..
Density 0.948 g/cc
0.0342 lb/in³
ISO 1183
Borealis BL1481 High Density Polyethylene
BL1481 is a semi high molecular weight polyethylene comprising an extra ordinary ESCR and very good chemical resistance This product is intended for blow molding. This grade is available in granular..
Density 0.948 g/cc
0.0342 lb/in³
ISO 1183
Unipetrol PE HD LITEN® FB 75 HDPE
Made for tubular film applications.Information provided by Unipetrol RPA
Density 0.948 g/cc
0.0342 lb/in³
ExxonMobil method
ExxonMobil Escorene™ UL 15028CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 15028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent..
Density 0.948 g/cc
0.0342 lb/in³
ExxonMobil method
ExxonMobil Escorene™ UL 40028CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 40028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent..
Density 0.948 g/cc
0.0342 lb/in³
ASTM D4883
ExxonMobil HDPE HD 8760.29 High Density Polyethylene Resin
Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal..
Density 0.948 g/cc
0.0342 lb/in³
Dow DOWLEX™ IP-42 High Density Polyethylene
DOWLEX® IP-42 resin is an improved processing high density polyethylene resin designed for excellent flow and high impact. DOWLEX IP-42 resin is designed by optimizing the breadth and shape of the ..
Density 0.947 g/cc
0.0342 lb/in³
ASTM D792
Dow DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE)
DOWLEX™ IP-51 is an Improved Processing high density resin designed to offer excellent process-ability and impact performance. This resin was designed by optimization of the breadth, shape and pea..
Density 0.948 g/cc
0.0342 lb/in³
ASTM D4883
ExxonMobil HDP8760.29 Rotational Molding Resin
Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal..
Density 0.947 g/cc
0.0342 lb/in³
ASTM-D792
Braskem GM7040G HDPE High Density Extrusion Polyethylene
GM7040G is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for a gas pressurized line. It is produced with bimodal technology and has high molar mass..
Density 0.947 g/cc
0.0342 lb/in³
ASTM D 792
Total CD 471 HDPE conduit
Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Density 0.948 g/cc
0.0342 lb/in³
ASTM D 792
Total Finathene® CD 481 HDPE conduit  (discontinued **)
Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
Amco PRIMATOP HDPE 003946HP Blow Molding Polyethylene
HDPE 003946HP features antistat, outstanding ESCR, and excellent impact resistance. Applications include detergent bottles, industrial containers, large parts, and household and industrial chemical ..
Density 0.946 g/cc
0.0342 lb/in³
Base; ASTM D792
Borealis Borstar® HE6062 HDPE Black Jacketing Compound
Borstar HE6062 is a black, bimodal co-polymer high density polyethylene (HDPE) compound produced using the Borealis Borstar process. It is characterized by balanced properties important in jacketin..