Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total Finathene® CD 481 HDPE conduit  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® CD 481 HDPE conduit  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D 792
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
ASTM D1693 cond. C 100% lgepal
High Load Melt Index 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D 2240
Tensile Strength, Yield >= 22.8 MPa
>= 3300 psi
ASTM D 638 type IV
Elongation at Break >= 800 %
>= 800 %
ASTM D 638 type IV
Flexural Modulus 0.862 GPa
125 ksi
ASTM D 790
Izod Impact, Notched 5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 180 µm/m-°C

@Temperature 20.0 °C
100 µin/in-°F

@Temperature 68.0 °F
ASTM D 696
Melting Point 129 °C
264 °F
ASTM D3417
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved