NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer NIZHNEKAMSKNEFTEKHIM Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Physical Properties Metric English Comments
Density 0.946 - 0.950 g/cc
0.0342 - 0.0343 lb/in³
Base Resin; ASTM D1505
Melt Flow 0.25 - 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.25 - 0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1283/L
4.5 - 7.2 g/10 min

@Load 21.6 kg,
Temperature 190 °C
4.5 - 7.2 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD >= 53.0 MPa
>= 7690 psi
ASTM D882
Film Tensile Strength at Yield, TD >= 50.0 MPa
>= 7250 psi
ASTM D882
Film Elongation at Break, MD >= 500 %
>= 500 %
ASTM D882
Film Elongation at Break, TD >= 650 %
>= 650 %
ASTM D882
Tensile Modulus >= 0.650 GPa
>= 94.3 ksi
2% sec, TD; ASTM D882
>= 0.700 GPa
>= 102 ksi
2% sec, MD; ASTM D882
Elmendorf Tear Strength, MD >= 0.709 g/micron
>= 18.0 g/mil
ASTM D1922
Elmendorf Tear Strength, TD >= 2.17 g/micron
>= 55.0 g/mil
ASTM D1922
Dart Drop Test >= 200 g
>= 0.441 lb
ASTM D1709
Descriptive Properties Value Comments
Gel Content (pcs./m²) 600