FS1470 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1470 have high impact and tensile strength, and balanced tear properties. Applications: heavy-duty sacks, refuse sacks and liners, and carrier-bag film. FS1470 contains antioxidant.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
ISO 1183
Melt Flow 0.20 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.20 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
6.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 250 %
250 %
ISO 527-3
Film Elongation at Break, TD 300 %
300 %
ISO 527-3
Tensile Modulus 1.00 GPa
145 ksi
MD; ASTM D882-A
1.10 GPa
160 ksi
TD; ASTM D882-A
Puncture Energy 1.50 J
1.11 ft-lb
45N; ASTM D5748
Dart Drop Test 350 g
0.772 lb
ISO 7765-1
Film Tensile Strength at Break, MD 50.0 MPa
7250 psi
ISO 527-3
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 130 °C
266 °F
ISO 11357-3
Vicat Softening Point 124 °C
255 °F
ISO 306
Processing Properties Metric English Comments
Melt Temperature 210 - 230 °C
410 - 446 °F