Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® HB-W747-A HDPE Extrusion Resin Molded Plaque Properties. Features: High molecular weight, excellent ESCR, impact strength, easy processing.Data provided by the manufacturer. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D1505 |
DuPont Elvax® 4320 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 4320 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications.ApplicationsElvax® 4320 resins can be used for the following applications: adhesives, s.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | Exxon Method |
ExxonMobil Escorene® UL-7505 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 19.2% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | Exxon Method |
ExxonMobil Escorene® UL-7720 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 28% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | Exxon Method |
ExxonMobil Escorene® MV-02520 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An experimental, very high flow, 20% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2607-UV14 HDPE Injection Molding Resin Excellent stiffness, Good impact resistance, Low warpageApplications: Roll-out cartsAdditives: Elevated levels of ultraviolet stabilizer packages, Elevated levels of antioxidantsInformation provided.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 8504 BK, 8504 GBK MDPE Rotational Molding Resin
(discontinued **) Features: Low melt index, excellent ESCR, high toughness at low temperatures.Applications: Large chemical storage tanks.Data provided by the manufacturer. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D1475 |
Humiseal 1C55 Silicone Conformal Coating Humiseal 1C55 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Density | 0.947 - 0.960 g/cc | 0.0342 - 0.0347 lb/in³ | ASTM D792 |
Forever Plast Namtene® Recycled Standard HDPE Standard Namtene® is used for dimple sheet, plastic slabs, and agricultural and construction applications. |
|||
Density | 0.947 - 0.953 g/cc | 0.0342 - 0.0344 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GF 5150 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ISO 1183/ISO 1872-2 |
Borealis VL4470 High Density Polyethylene VL4470 is a high density polyethylene. Applications: Blown film, Rashel knitted and woven fabrics, and Stretch tape.Information provided by Borealis AG |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D 792 |
Total CD 4300 HDPE extrusion Applications: General profile extrusion, irradiation-crosslinked productsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ISO 1183 |
Borealis FS1470 High Density Polyethylene FS1470 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1470 have high impact and tensile strength, and bala.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
DuPont Bynel® 1124 Modified EVA Adhesive Resin Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
Total HL 428 HDPE Film Grade Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
Dow DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE) DOWLEX™ IP-51 is an Improved Processing high density resin designed to offer excellent process-ability and impact performance. This resin was designed by optimization of the breadth, shape and pea.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM-D792 |
Braskem GM7040G HDPE High Density Extrusion Polyethylene GM7040G is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for a gas pressurized line. It is produced with bimodal technology and has high molar mass.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | |
Axion Polymers Axpoly® HDPE12 1000 High Purity Molding Produced from 100% post-consumer raw materials, this product fits closely with Axion's other recycled resin grades and offers the same set of user benefits, including:Successfully replaces virgin re.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | |
Axion Polymers Axpoly® HDPE21 1000 High Purity Molding Produced from 100% post-consumer raw materials, this product fits closely with Axion's other recycled resin grades and offers the same set of user benefits, including:Successfully replaces virgin re.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | |
3M Hi-Strength 94 ET Adhesive A high performance, industrial grade spray adhesive with a unique low telegraphing pebble spray pattern.Features:Bonds to a variety of substrates including decorative laminate, headliners, and soft .. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | |
3M Scotch-Weld™ Hi-Strength Postforming 94 CA Cylinder Spray Adhesive A low VOC, high performance, postformable grade spray adhesive with a unique low telegraphing pebble spray pattern.Features:Bonds to a variety of demanding substrates like decorative laminate, metal.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | Part B |
Abatron AboCast 8103-23 High-Performance Dielectric Epoxy AboCast 8103-23 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has a comb.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2607-UV9 HDPE Injection Molding Resin
(discontinued **) Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D 792 |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | Exxon Method |
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It produces a so.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | ASTM D1505 |
Braskem HF 0147 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |
|||
Density | 0.947 g/cc | 0.0342 lb/in³ | AboCure 7606-1 |
Abatron AboCast/AboCure 7606-1 Epoxy AboCast 7606-1 is a transparent, light amber resin with a weight of 9.5 lbs/gallon and a viscosity of 2100 cps approx. @ 25°C. AboCure 7606-1 is a transparent, light amber converter with a weight o.. |
|||
Density | 0.947 - 1.10 g/cc | 0.0342 - 0.0397 lb/in³ | Average value: 1.00 g/cc Grade Count:18 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |