Material Notes:
K46-06-185 is a natural high molecular weight, high-density copolymer polyethylene developed for automotive fuel tanks. It combines excellent processability and outstanding physical performance, particularly environmental stress crack resistance (ESCR) and impact properties. Its high melt strength aids the continuous extrusion production of multi-layer tanks.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D4883
High Load Melt Index 4.2 g/10 min
4.2 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Yield 23.4 MPa
3390 psi
2 in/min.; ASTM D638
Elongation at Break 800 %
800 %
2 in/min.; ASTM D638
Flexural Modulus 0.820 GPa
119 ksi
2% Secant; ASTM D790
Izod Impact, Notched 3.75 J/cm
7.03 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C
156 °F
ASTM D648
Vicat Softening Point 129 °C
264 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Extrusion
Region US & Canada
Bamberger Polymers Distribution