Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene® HD-8761 LHDPE Rotational Molding Grade  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Rotational Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® HD-8761 LHDPE Rotational Molding Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.HD-8700 series are linear high density polyethylene resins that provide outstanding environmental stress crack resistance. HD-8761 is fully formulated long term UV stability package in ground form.Applications: Recreational products; Industrial components; RV tanks.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
Exxon Method
Environmental Stress Crack Resistance 8.0 hour
8.0 hour
F50, Condition B; ASTM D-1693
Melt Flow 5.0 g/10 min
5.0 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break 405 %
405 %
ASTM D638
Flexural Modulus 0.930 GPa
135 ksi
ASTM D790
Impact Test 203 J

@Thickness 6.35 mm,
Temperature -40.0 °C
150 ft-lb

@Thickness 0.250 in,
Temperature -40.0 °F
Impact Strength; Max Force; ARM
Thermal Properties Metric English Comments
Melting Point 133 °C
271 °F
Exxon Method
Deflection Temperature at 0.46 MPa (66 psi) 57.0 °C
135 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C
108 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved